Effect of ferric nitrate loading mode on properties of Si3N4 composite MgO-C refractories prepared by nitridation

Chen Yang, Deng Chengji, Ding Jun, Yu Chao, Lou Xiaoming   

  1. Research Institute of New Building Materials,Hunan Institute of Technology,Heng-yang 421002,Hunan,China
  • Received:2021-01-13 Online:2022-12-15 Published:2022-12-26

硝酸铁负载方式对氮化制备Si3N4复合MgO-C材料的影响

陈洋1,2), 邓承继2), 丁军2), 余超2), 娄晓明1)   

  1. 1)湖南工学院 新型建筑材料研究院 湖南衡阳 421002
    2)武汉科技大学 省部共建耐火材料与冶金国家重点实验室 湖北武汉 430081
  • 作者简介:陈洋:男,1992年生,博士。E-mail:chenyang_9210@163.com
  • 基金资助:
    国家自然科学基金区域创新发展联合基金(U20A20239);湖北省自然科学基金面上项目(2020CFB692)和湖南省教育厅重点项目(18A428)联合资助。

Abstract: In order to investigate the effect of the catalyst loading mode on the mechanical properties of Si3N4 composite MgO-C refractories prepared by nitridation,fused magnesia,flake graphite,silicon powder,and phenolic resin were used as the main raw materials,and ferric nitrate as the catalyst to prepare refractories by nitriding at 1 350 ℃.The effects of different catalyst supports (silicon powder,silicon powder+phenolic resin) on the formation of Si3N4 in MgO-C refractories and the properties of refractories were studied.The results show that the silicon powder+phenolic resin catalyst support promotes the participation of α-Si3N4 in the reaction to generate β-Si3N4 and MgSiN2,and generates more SiC.However,this loading mode causes more gas to escape from the refractories and loosens the material structure,which reduces the mechanical properties.On the contrary,MgO-C refractories prepared by nitridation with silicon powder-supported catalysts under the same conditions show higher density and better mechanical properties.

Key words: magnesia-carbon refractories, catalyst support, silicon nitride, mechanical properties

摘要: 为了探明催化剂负载方式对氮化制备Si3N4复合MgO-C耐火材料力学性能的影响,以电熔镁砂、鳞片石墨、硅粉、酚醛树脂为主要原料,以硝酸铁为催化剂,经1 350 ℃氮化制备了Si3N4复合MgO-C耐火材料,研究了不同催化剂载体(硅粉、硅粉+酚醛树脂)对MgO-C耐火材料中Si3N4的形成和材料性能的影响。结果表明:采用硅粉+酚醛树脂为催化剂载体,会促进α-Si3N4参与反应生成β-Si3N4和MgSiN2,并提高SiC生成量,但这种负载方式会导致试样内部产生较多气体而逸出,材料结构变得疏松,降低了材料的力学性能;相同条件下硅粉负载催化剂氮化制备MgO-C耐火材料显示出更高的致密度和力学性能。

关键词: MgO-C耐火材料, 催化剂载体, Si3N4, 力学性能