Synthesis methods and applications of hexagonal boron nitride powders and nanosheets
Huang Yucan, Shen Jiajie, Guan Chengzhi, Long Dewu
Refractories . 2025, (
3
): 266 -270 . DOI: 10.3969/j.issn.1001-1935.2025.03.016