耐火材料 ›› 2025, Vol. 59 ›› Issue (1): 1-7.DOI: 10.3969/j.issn.1001-1935.2025.01.001

• 研究开发 •    下一篇

Si3N4/Si2N2O复相粉体对Al2O3-SiC-C浇注料性能的影响

李有奇1), 何健1), 陈俊峰2), 张嘉良1), 李正坤1)   

  1. 1)江苏晶鑫新材料股份有限公司 江苏扬州 225000
    2)武汉科技大学 省部共建耐火材料与冶金国家重点实验室 湖北武汉 430081
  • 收稿日期:2024-05-29 出版日期:2025-02-15 发布日期:2025-02-27
  • 作者简介:* 李有奇:男,1979年生,博士。E-mail:13348121669@163.com

Effect of Si3N4/Si2N2O multiphase powder on properties of Al2O3-SiC-C castables

Li Youqi, He Jian, Chen Junfeng, Zhang Jialiang, Li Zhengkun   

  1. First author’s address:Jiangsu Jingxin New Materials Co.,Ltd.,Yangzhou 225000,Jiangsu,China
  • Received:2024-05-29 Online:2025-02-15 Published:2025-02-27

摘要: 为了提高Al2O3-SiC-C浇注料的综合服役性能,采用化学燃烧法合成的微晶氮化硅/氮氧化硅(Si3N4/Si2N2O)复相粉体为添加物,以棕刚玉、板状刚玉、碳化硅、活性α-Al2O3微粉、SiO2微粉、纯铝酸钙水泥、单质Si粉和球沥青为原料,制备了Al2O3-SiC-C浇注料。研究了复相粉体外加量(外加质量分数分别为0、1%、2%、3%和5%)对浇注料性能的影响,同时探究Si3N4/Si2N2O增强试样综合性能的作用机制。结果表明:1)Si3N4/Si2N2O复相粉可以显著改善Al2O3-SiC-C浇注料的力学性能、抗氧化性能和抗热震性;2)Si3N4/Si2N2O 复相粉通过填充孔隙、促进烧结反应进行、生成晶须状物质等途径优化了浇注料的显微结构,提高了浇注料的综合性能;3)当Si3N4/Si2N2O复相粉外加量为3%(w)时,浇注料的性能最佳。

关键词: Si3N4/Si2N2O复相粉, Al2O3-SiC-C浇注料, 抗氧化性, 抗热震性

Abstract: In order to improve the comprehensive service performance of Al2O3-SiC-C castables,microcrystalline Si3N4/Si2N2O multiphase powder synthesized by chemical combustion was used as an additive to prepare Al2O3-SiC-C castables,using brown corundum,tabular corundum,silicon carbide,active α-Al2O3 micropowder,SiO2 micropowder,pure calcium aluminate cement,Si powder,and ball asphalt as raw materials.The effect of the multiphase powder extra-addition (0,1%,2%,3%,and 5%,by mass) on properties of the castables was studied;and the mechanism of Si3N4/Si2N2O to enhance the comprehensive properties of the samples was explored.The results show that:(1)Si3N4/Si2N2O multiphase powder can significantly improve the mechanical properties,oxidation resistance,and thermal shock resistance of the Al2O3-SiC-C castables;(2)the Si3N4/Si2N2O multiphase powder optimizes the microstructure of the castable and improves its overall performance by filling pores,promoting sintering reactions,and generating whisker like substances;(3)when the Si3N4/Si2N2O multiphase powder extra-addition is 3%,the castable has the optimal performance.

Key words: Si3N4/Si2N2O multiphase powder, Al2O3-SiC-C castable, oxidation resistance, thermal shock resistance