耐火材料 ›› 2025, Vol. 59 ›› Issue (3): 229-233.DOI: 10.3969/j.issn.1001-1935.2025.03.009

• 生产应用 • 上一篇    下一篇

烧结温度对微量Al2O3添加Mg-PSZ陶瓷性能的影响

刘雨佳, 刘涛, 韩磊   

  1. 东北大学 冶金学院 辽宁沈阳 110819
  • 收稿日期:2024-11-08 出版日期:2025-06-15 发布日期:2025-06-16
  • 通讯作者: 刘涛,男,1976年生,教授,博士生导师。E-mail:liut@smm.neu.edu.cn
  • 作者简介:刘雨佳:女,1999年生,硕士研究生。E-mail:lyj20220202@163.com
  • 基金资助:
    国家自然科学基金资助项目(51974072)。

Effect of sintering temperatures on properties of Mg-PSZ ceramics added with trace Al2O3 addition

Liu Yujia, Liu Tao, Han Lei   

  1. First author’s address:School of metallurgy,Northeastern University,Shenyang 110819,Liaoning,China
  • Received:2024-11-08 Online:2025-06-15 Published:2025-06-16

摘要: 为了研究微量Al2O3添加对Mg-PSZ粉体烧结活性和陶瓷性能的影响,以ZrO2、MgO和Al2O3为原料,固相烧结合成微量Al2O3添加的氧化镁部分稳定氧化锆(Mg-PSZ)陶瓷试样,与未添加Al2O3的Mg-PSZ试样进行比较分析。研究烧结温度(1 000~1 700 ℃保温2 h,间隔100 ℃)对试样物相组成、显微结构、性能的影响。结果表明:1)随烧结温度的升高,2种试样中c-ZrO2和t-ZrO2相的含量均增加,离子电导率均增加,但未添加Al2O3的试样的体积密度增加,而添加Al2O3的试样的体积密度先增加后减小;2)添加Al2O3的试样的综合性能比未添加Al2O3的试样的好;3)添加Al2O3的试样经1 600 ℃烧后的综合性能最好。

关键词: Mg-PSZ陶瓷, 微量Al2O3, 常温耐压强度, 离子电导率

Abstract: In order to study the effect of a trace Al2O3 addition on the properties of Mg-PSZ ceramics,MgO partially stabilized zirconia (Mg-PSZ) ceramic samples with trace Al2O3 were synthesized by solid-state sintering using ZrO2,MgO,and Al2O3 as raw materials,and compared with Mg-PSZ samples without Al2O3.The effects of sintering temperatures (1 000-1 700 ℃ for 2 h with an interval of 100 ℃) on the phase composition,microstructure,properties of the samples were studied.The results show that:(1)with the sintering temperature rising,the total contents of c-ZrO2 and t-ZrO2 phases in the two samples both increase,the ionic conductivity increases;however,the bulk density of the sample without Al2O3 increases,while that of the samples with Al2O3 increases first and then decreases;(2)the comprehensive performance of the sample with Al2O3 is better than that without Al2O3;(3)the sample with Al2O3 has the best comprehensive performance after firing at 1 600 ℃.

Key words: Mg-PSZ ceramics, trace Al2O3, cold compressive strength, ionic conductivity

中图分类号: