耐火材料 ›› 2025, Vol. 59 ›› Issue (1): 54-58.DOI: 10.3969/j.issn.1001-1935.2025.01.010

• 生产应用 • 上一篇    下一篇

利用铁尾矿制备莫来石材料的研究

孙家朐1), 刘新1), 丁璇1), 吴锋1), 罗旭东1,2)   

  1. 1)辽宁科技大学 材料与冶金学院 辽宁鞍山 114051
    2)辽宁科技学院 辽宁本溪 117004
  • 收稿日期:2024-05-22 出版日期:2025-02-15 发布日期:2025-02-27
  • 通讯作者: 刘新,女,1980年生,博士,讲师。E-mail:lxkdgm@163.com
  • 作者简介:孙家朐:男,1999年生,硕士研究生。E-mail:sunjj@ustl.edu.cn
  • 基金资助:
    * 国家自然科学基金(U20A20239)。

Preparation of mullite materials with iron tailings

Sun Jiaqu, Liu Xin, Ding Xuan, Wu Feng, Luo Xudong   

  1. First author’s address:School of Materials and Metallurgy,University of Science and Technology Liaoning,Anshan 114051,Liaoning,China
  • Received:2024-05-22 Online:2025-02-15 Published:2025-02-27

摘要: 为提升铁尾矿的综合利用率,以铁尾矿为硅源,Al(OH)3为铝源,通过固相反应烧结法制备莫来石材料,研究了热处理温度(1 250、1 300、1 350和1 400 ℃保温3 h)对莫来石材料微观形貌及烧结性能的影响。结果表明:1)铁尾矿中的Fe3+在固相反应过程中可以部分取代莫来石中的Al3+形成含铁莫来石固溶体,导致晶格常数增大,使莫来石衍射峰向小角度偏移;2)热处理温度的升高使得体系中液相增多,莫来石形貌由颗粒状逐渐生长成柱状;3)经1 350 ℃热处理3 h可以制备出综合性能优异的莫来石材料,其显气孔率为18.2%,体积密度为2.53 g·cm-3,常温抗折强度为58.8 MPa。

关键词: 铁尾矿, 莫来石, 氢氧化铝, 烧结性能

Abstract: To enhance the comprehensive utilization of iron tailings,mullite materials were prepared by the solid state reaction sintering method using iron tailings as the silicon source and Al(OH)3 as the aluminium source.The effects of heat treatment temperatures (1 250,1 300,1 350 and 1 400 ℃ for 3 h) on the microscopic morphology and sintering properties of the mullite materials were investigated.The results show that:(1)Fe3+ in the iron tailings can partially replace Al3+ in mullite to form an iron-containing mullite solid solution during the solid state reaction,which leads to an increase in the lattice constant and a shift of mullite diffraction peaks to small angles;(2)increasing the heat treatment temperature produces more liquid phases in the system,and mullite grows gradually from granular to columnar;(3)after the heat treatment at 1 350 ℃ for 3 h,a mullite material with excellent comprehensive properties can be obtained with the apparent porosity of 18.2%,bulk density of 2.53 g·cm-3 and cold modulus of rupture of 58.8 MPa.

Key words: iron tailings, mullite, aluminum hydroxide, sintering properties