Preparation of MgB2O5 whiskers from reverse flotation magnesite tailings

Dong Zeming, Dong Zeguang, Wang Shuxing, Liu Zhaoyang   

  1. First author’s address:Shenyang Aircraft Corporation,Shenyang 110850,Liaoning,China
  • Received:2024-10-14 Online:2025-06-15 Published:2025-06-16

摘要: 为了提高菱镁矿尾矿的回收利用,且寻找一种环保的镁源制备MgB2O5晶须,以反浮选菱镁矿尾矿作为镁源,利用熔盐法合成Mg2B2O5晶须。研究了尾矿活化处理、反应温度(700、800和900 ℃)以及硼酸与尾矿质量比(定义为硼镁比,分别为0.62、1.24、1.86和2.48)对Mg2B2O5晶须物相组成和显微结构的影响。结果表明:Mg2B2O5晶须的长径比随着硼镁比的增加先增加后减小,当硼镁比为1.86时,达到最大值;800 ℃为MgB2O5晶须生长的最佳温度,低于此温度难以生成晶须,而温度过高则会导致晶须粗化,长径比减小;球磨和轻烧处理菱镁矿尾矿可破坏尾矿分解后存在的母盐假相,减小粒径,从而提高镁源活性,以此为镁源可获得尺寸均匀和高长径比的Mg2B2O5晶须。

关键词: MgB2O5晶须, 熔盐法, 母盐假相, 长径比

Abstract: Using reverse flotation magnesite tailings as a magnesium source,Mg2B2O5 whiskers were synthesized via a molten salt method in order to improve the recycling utilization of magnesite tailings and find an environmental friendly magnesium source for MgB2O5 whiskers.The effects of the tailings activating treatment,reaction temperature (700,800 and 900 ℃),and mass ratio of boric acid to magnesite tailings (B/Mg mass ratio=0.62,1.24,1.86 or 2.48) on the phase composition and microstructure of the whiskers were investigated.The results indicate that the aspect ratio of Mg2B2O5 whiskers initially increases and then decreases with the B/Mg mass ratio increasing,reaching the maximum value at a ratio of 1.86.Furthermore,800 ℃ is identified as the optimal temperature for the growth of Mg2B2O5 whiskers; whisker formation is difficult below this temperature,while excessively high temperatures lead to whisker coarsening and a reduction in the aspect ratio.The ball milling and light burnt treatment of the magnesite tailings can disrupt pseudomorph after decomposition,and reduce the particle size,thereby enhancing the activity of the magnesium source and yielding uniform-sized Mg2B2O5 whiskers with a high aspect ratio.

Key words: Mg2B2O5 whiskers, molten salt method, pseudomorph, aspect ratio