耐火材料 ›› 2026, Vol. 60 ›› Issue (5): 397-401.DOI: 10.3969/j.issn.1001-1935.2026.05.005

• 研究开发 • 上一篇    下一篇

镁锆粉对刚玉-尖晶石质浇注料性能的影响

雷宇湉1,2), 聂建华1,2), 陈瑞峰3), 张小旭3), 梁永和1,2,3)   

  1. 1)武汉科技大学 先进耐火材料全国重点实验室 湖北武汉 430081
    2)武汉科技大学 钢铁工业耐火材料新技术教育部国际合作联合实验室 湖北武汉 430081
    3)洛阳轩石新材料科技有限公司 河南洛阳 471800
  • 收稿日期:2025-12-18 出版日期:2026-10-15 发布日期:2026-10-29
  • 通讯作者: 聂建华,男,1974年生,博士,副教授。E-mail:niejianhua@wust.edu.cn
  • 作者简介:雷宇湉:女,1997年生,硕士研究生。E-mail:1225904613@qq.com
  • 基金资助:
    国家自然科学基金联合基金重点项目(U21A2058);湖北省中央引导地方科技发展专项(2025CSA017)。

Effect of magnesia-zirconia powder on properties of corundum-spinel based castables

Lei Yutian, Nie Jianhua, Chen Ruifeng, Zhang Xiaoxu, Liang Yonghe   

  1. First author’s address:The State Key Laboratory of Advanced Refractories,Wuhan University of Science and Technology,Wuhan 430081,China
  • Received:2025-12-18 Online:2026-10-15 Published:2026-10-29

摘要: 为了开发高性能无铬透气砖,以板状刚玉、烧结刚玉、纯铝酸盐水泥、镁锆粉以及预混合细粉(尖晶石粉、板状刚玉、白刚玉、富铝尖晶石粉和α-Al2O3微粉)为原料,制备了刚玉-尖晶石质浇注料,探讨了镁锆粉加入量(加入质量分数分别为0、0.5%、1.0%、1.5%、2.0%、2.5%、3.0%和3.5%)对刚玉-尖晶石质浇注料常温物理性能及抗热震性能的影响。结果表明:1 550 ℃热处理后,随着镁锆粉加入量的增多,ZrO2能均匀地分布在基质中,MgAl2O4及CA6在基质中与ZrO2穿插结合,结构更加致密,加热永久线变化降低,试样的强度提高;此外,加入一定量的镁锆粉可以明显改善试样的抗热震性,镁锆粉加入量为3.5%(w)试样的常温抗折强度保持率高达63%,较未添加镁锆粉试样的明显提升。综合各项性能及成本考虑,镁锆粉加入量为3.5%(w)的浇注料配比制备的透气砖在LF精炼钢包上试用,其与钢厂现用含铬透气砖的使用寿命基本相当,达48~50次。

关键词: 镁锆粉, 浇注料, 刚玉-尖晶石质, 抗热震性

Abstract: To develop high-performance chrome-free purging plugs,corundum-spinel castables were prepared using tabular corundum,sintered corundum,pure calcium aluminate cement,magnesia-zirconia powder,and premixed fine powders (spinel powder,tabular corundum,white corundum,alumina-rich spinel powder,and α-Al2O3 micropowder) as raw materials.The effects of magnesia-zirconia powder addition (0,0.5%,1.0%,1.5%,2.0%,2.5%,3.0%,and 3.5%,by mass) on the cold physical properties and thermal shock resistance of the corundum-spinel castables were investigated.The results show that after the heat treatment at 1 550 ℃,with the increasing magnesia-zirconia powder addition,ZrO2 is uniformly distributed in the matrix;MgAl2O4 and CA6 interlock with ZrO2 in the matrix,making the structure denser;the permanent linear change decreases;and the strength of the samples increases.In addition,adding an appropriate amount of magnesia-zirconia powder significantly improves the thermal shock resistance of the samples.For the sample with 3.5% magnesia-zirconia powder,the retention ratio of the cold modulus of rupture reaches 63%,which is significantly higher than that of the sample without magnesia-zirconia powder.Considering overall performance and cost,the purging plug prepared with the castable formulation containing 3.5% magnesia-zirconia powder was trial-used in an LF refining ladle.Its service life was basically comparable to that of the chrome-containing purging plugs currently used in the steel plant,reaching 48-50 heats.