Effects of calcium aluminate cement addition on fracturing proppant

Zhang Mengzhen1)(), Lu Xinyu2), Yin Rui1), Zhang Guoqiang3), Guo Lipeng3)   

  1. 1)Henan Building Materials Research and Design Institute Co.,Ltd.,Zhengzhou 450002,Henan,China
  • Received:2020-10-12 Online:2021-04-15 Published:2021-04-15

铝酸钙水泥添加量对压裂支撑剂的影响

张梦真1)(), 陆昕昱2), 尹蕊1), 张国强3), 郭利朋3)   

  1. 1)河南建筑材料研究设计院有限责任公司 河南郑州 450002
    2)中国中化集团有限公司创新与战略发展部 北京 100031
    3)洛阳赛罗帕陶瓷科技有限公司 河南洛阳 471133
  • 作者简介:张梦真:女,1990年生,工程师。E-mail:1179739123@qq.com
  • 基金资助:
    河南省科研开发专项(豫科院2019101)

Abstract:

Fracturing proppant was prepared using second grade bauxite powder as the main starting material,ceramic proppant waste powder as the auxiliary raw material,adding 1 mass%-4 mass% of calcium aluminate cement (CA50) as additive,granulating into balls,drying,and firing.The influences of the CA50 addition on properties of the proppant samples such as the bulk density,the breakage ratio and the acid solubility were determined;meanwhile,XRD,and SEM and EDS analyses were conducted.The results show that (1)no mullite is detected,the samples mainly contain corundum,iron-aluminium titanate (FeAlTiO5),anorthite,and glass;as the CA50 addition increases,corundum and FeAlTiO5 decrease,anorthite and glass increase;(2)with the increasing CA50 addition,the bulk density and the crushing resistance of the sintered samples first increase and then decrease,and the maximum value appears with 3 mass% CA50;3)with the increasing CA50 addition,the acid solubility of the sintered samples increases gradually,indicating that the resistance to acid solution erosion keeps declining.

Key words: calcium aluminate cement, fracturing proppant, bulk density, apparent density, acid solubility, phase composition

摘要:

以二级铝矾土细粉为主要原料,陶粒支撑剂废品细粉为辅助原料,同时添加0~4%(w)的铝酸钙水泥(CA50),经制粒成球、干燥、烧成等制成压裂支撑剂试样。考察了CA50加入量对支撑剂试样体积密度、破碎率、酸溶解度等性能的影响,并进行了XRD、SEM、EDS分析。结果表明:1)烧成试样中未检测到莫来石,主要由刚玉、铁铝钛酸盐固溶体(FeAlTiO5)、钙长石和玻璃相组成;且随着CA50加入量的增加,刚玉相和FeAlTiO5逐渐减少,钙长石相和玻璃相逐渐增多。2)随着CA50加入量的增加,烧成试样的体积密度和抗破碎能力呈先增大后减小的变化趋势,添加3%(w)的CA50时最大。3)随着CA50加入量的增加,烧成试样的酸溶解度逐渐增大,表明其抵抗酸溶液侵蚀的能力持续下降。

关键词: 铝酸钙水泥, 压裂支撑剂, 体积密度, 视密度, 酸溶解度, 物相组成