Refractories ›› 2022, Vol. 56 ›› Issue (2): 166-169.DOI: 10.3969/j.issn.1001-1935.2022.02.016

Previous Articles     Next Articles

Influence of lightweight aggregates type on properties of high alumina castables

Guo Wenhui1,2)(), Bo Jun2)(), Yuan Bo1), Hao Xian1), Zhang Lei1), Luo Tian1)   

  1. 1)State Key Laboratory of Advanced Refractories,Sinosteel Luoyang Institute of Refractories Research Co.,Ltd.,Luoyang 471039,Henan,China
  • Received:2021-10-26 Online:2022-04-15 Published:2022-04-21
  • Contact: Bo Jun

轻质骨料种类对高铝浇注料性能的影响

郭文辉1,2)(), 薄钧2)(), 袁波1), 郝娴1), 张雷1), 罗天1)   

  1. 1)中钢集团洛阳耐火材料研究院有限公司 先进耐火材料国家重点实验室 河南洛阳 471039
    2)中钢洛耐科技股份有限公司 河南洛阳 471003
  • 通讯作者: 薄钧
  • 作者简介:郭文辉:男,1993年生,硕士研究生。E-mail: vipgwh@163.com

Abstract:

In order to reduce their bulk density and thermal conductivity,three kinds of high alumina castables were prepared with lightweight microporous mullite,porous high alumina clinker and alumina bubbles as aggregates,respectively,and their properties after drying and heat treatment at 1 250 ℃ were studied.The results show that:(1)the drying strength of the castables mainly depends on the strength of the lightweight aggregates used,and the strength after heat treatment at 1 250 ℃ is also related to the sintering degree of the castables;the thermal conductivity is mainly affected by the density of aggregates as well as the size and distribution of pores;(2)the castable prepared with the lightweight microporous mullite as the aggregates has higher cold strength and hot modulus of rupture,and lower thermal conductivity.

Key words: lightweight aggregates, lightweight castables, high alumina castables, bulk density, thermal conductivity

摘要:

为了降低高铝浇注料的体积密度和热导率,研究了分别以轻质微孔莫来石、高铝多孔熟料和氧化铝空心球为骨料的三种高铝浇注料的烘干及1 250 ℃热处理后的性能。结果表明:1)浇注料的烘干强度主要取决于所用轻质骨料的强度,1 250 ℃热处理后的强度还与浇注料的烧结程度有关;热导率主要受骨料的致密度以及气孔的大小和分布影响。2)比较后发现,以轻质微孔莫来石为骨料制备的浇注料的常温强度和高温抗折强度较大,热导率较低。

关键词: 轻质骨料, 轻质浇注料, 高铝浇注料, 体积密度, 热导率

CLC Number: