Refractories ›› 2021, Vol. 55 ›› Issue (4): 329-331.DOI: 10.3969/j.issn.1001-1935.2021.04.013

Previous Articles     Next Articles

Application of dry desulphurization and SCR denitrification technology in flue gas treatment of tunnel kilns for firing magnesia-calcia brick

Chen Jing(), Zhang Jie, Deng Yunbo, Lu Yike, Liu Xin, Zhang Yi   

  1. Beijing ZHTY Technology Co.,Ltd.,Beijing 100041,China
  • Received:2020-10-30 Online:2021-08-15 Published:2021-08-22

干法脱硫、SCR脱硝在镁钙砖烧成用隧道窑烟气治理中的应用

陈晶(), 张杰, 邓云波, 卢一科, 刘欣, 张艺   

  1. 北京中航天业科技有限公司 北京 100041

Abstract:

Taking the flue gas treatment of tunnel kilns for firing magnesia-calcia brick as an example,the treatment process of dry desulphurization and SCR denitrification technology was put forward.The ultra-low emission standards of sulfur dioxide,dust and nitrogen oxide lower than 10,35 and 50 mg·m-3,respectively were realized.The process has been put into use in a magnesia-calcia brick enterprise in Shanxi Province,and the operation effect was good,but the cost of per ton product increased about CNY13.5.

Key words: dry desulphurization, SCR denitrification, magnesia-calcia brick, tunnel kilns, ultra-low emi-ssion

摘要:

以镁钙砖烧成用隧道窑烟气治理为例,提出了干法脱硫、选择性催化还原(简称SCR)脱硝的治理工艺。据此,可以实现二氧化硫、粉尘和氮氧化物的排放浓度分别低于10、35和50 mg·m-3的超低排放标准。该工艺已在山西某生产镁钙砖的耐火材料企业投入使用,运行效果良好,但每吨产品增加成本约13.5元。

关键词: 干法脱硫, SCR脱硝, 镁钙砖, 隧道窑, 超低排放