Refractories ›› 2022, Vol. 56 ›› Issue (6): 489-494.DOI: 10.3969/j.issn.1001-1935.2022.06.007

Previous Articles     Next Articles

Effect of TiO2 addition on performance of Al2O3-SiC-C taphole clay

Ju Maoqi, Liang Yonghe, Nie Jianhua, Cai Manfei, Guo Mengzhen   

  1. The State Key Laboratory of Refractories and Metallurgy,Wuhan University of Science and Technology,Wuhan 430081,Hubei,China
  • Received:2022-02-07 Online:2022-12-15 Published:2022-12-26

TiO2添加量对Al2O3-SiC-C质炮泥性能的影响

鞠茂奇, 梁永和, 聂建华, 蔡曼菲, 郭梦真   

  1. 武汉科技大学 材料与冶金学院 湖北武汉 430081
  • 通讯作者: 梁永和,男,1959年生,博士,教授。E-mail:wkdlyh@126.com
  • 作者简介:鞠茂奇:男,1995年生,博士研究生。E-mail:624185197@qq.com

Abstract: In order to improve the properties of Al2O3-SiC-C taphole clay,the effects of TiO2 additions (0,1%,2%,3%,and 4%,by mass) on the performance of samples after hot treatment were studied,including the permanent linear change,the density,the cold strength,the oxidation resistance and the slag resistance,etc.The results show that:(1)after heat treatment at 1 100 ℃ for 3 h,all samples shrink and the linear shrinkage rate increases with the TiO2 addition increasing,the density and the cold strength also increase with the increase of TiO2 addition;(2)after heat treatment at 1 450 ℃ for 3 h,all samples expand due to the volume expansion caused by the formation of mullite;with the TiO2 addition increasing,the linear expansion rate increases,the density decreases,and the cold strength increases first and then decreases and reaches the maximum with 3% of TiO2;(3)adding TiO2,the oxidation resistance and the slag corrosion resistance of the taphole clay are slightly improved.

Key words: titania, taphole clay, alumina-silicon carbide-carbon, density, cold strength, corrosion resistance

摘要: 为了提高Al2O3-SiC-C质炮泥的性能,研究了TiO2添加量(质量分数分别为0、1%、2%、3%、4%)对Al2O3-SiC-C质炮泥热处理后烧后线变化、致密度、常温强度、抗氧化性和抗渣性等性能的影响。结果表明:1)在1 100 ℃保温3 h热处理后,试样均发生收缩,其线收缩率随TiO2的增多而增大;试样的致密度和常温强度也均随TiO2的增多而增大。2)在1 450 ℃保温3 h热处理后,由于试样中莫来石的生成伴随体积膨胀,试样均发生膨胀,其线膨胀率随TiO2的增多而增大;试样的致密度随TiO2的增多而减小;试样的常温强度随TiO2的增多呈先增大后减小的变化趋势,在TiO2添加量为3%(w)时达到最大。3)添加TiO2后,炮泥的抗氧化性和抗渣侵蚀性均略有改善。

关键词: TiO2, 炮泥, Al2O3-SiC-C, 致密度, 常温强度, 抗侵蚀性