Refractories ›› 2023, Vol. 57 ›› Issue (4): 305-309.DOI: 10.3969/j.issn.1001-1935.2023.04.007

Previous Articles     Next Articles

Corrosion of Li(NixCoyMnz)O2 cathode materials to KAlSi2O6 prepared via sol-gel method

Ma Junhua, Luo Zhongtao, Li Ye, Jia Quanli, Mu Yuandong, Chen Liugang   

  1. First author’ s address:Henan Key Laboratory of High Temperature Functional Ceramics,Zhengzhou University,Zhengzhou 450052,Henan,China
  • Received:2023-01-28 Online:2023-08-15 Published:2023-08-30

Li(NixCoyMnz)O2正极材料对溶胶-凝胶法制备KAlSi2O6的侵蚀研究

马俊花, 罗忠涛, 李烨, 贾全利, 穆元冬, 陈留刚   

  1. 郑州大学 河南省高温功能材料重点实验室 河南郑州 450052
  • 作者简介:马俊花:女,1996年生,硕士研究生。E-mail:202022192013716@gs.zzu.edu.cn
  • 基金资助:
    国家自然科学基金(51802287);河南省重点研发与推广专项(212102210593)。

Abstract: KAlSi2O6(KAS4) sol with or without CaF2 was calcined at 800-1 300 ℃ to obtain KAS4 powder.The obtained KAS4 powder and CaF2 powder were uniformly mixed with Li(NixCoyMnz)O2 (LNCM) materials in the mass ratio of 70∶30,and then held at 1 100 ℃ for 6 h for corrosion tests.The phase composition of KAS4 without or with CaF2 as well as the phase composition and microstructure after corrosion tests were compared and analyzed.The results illustrate that:(1)1.88 mass% CaF2 addition reduces the forming temperature of KAS4 pure phase by approximately 100 ℃;(2)CaF2-free KAS4 exhibits better corrosion resistance to LNCM compared with CaF2-containing KAS4;(3)CaF2 is easy to react with LNCM at high temperatures.

Key words: sol-gel method, KAlSi2O6, Li(NixCoyMnz)O2, corrosion resistance

摘要: 将不加和添加CaF2的KAlSi2O6(KAS4)溶胶于800~1 300 ℃煅烧得到的KAS4以及原料CaF2粉,分别与Li(NixCoyMnz)O2(LNCM)按照质量比70∶30混合均匀,然后在1 100 ℃保温6 h进行侵蚀试验。对比分析了不加和添加CaF2的KAS4的物相组成以及侵蚀试验后几种材料的物相组成和显微结构。结果表明:1)添加 1.88%(w)CaF2可以使KAS4纯相的生成温度下降约100 ℃;2)不加CaF2的KAS4比添加CaF2的具有更好的抗LNCM侵蚀性能;3)CaF2与LNCM在高温下容易发生反应。

关键词: 溶胶-凝胶法, KAlSi2O6, Li(NixCoyMnz)O2, 抗侵蚀性