Refractories ›› 2023, Vol. 57 ›› Issue (4): 310-313.DOI: 10.3969/j.issn.1001-1935.2023.04.008

Previous Articles     Next Articles

Effect of B4C addition on properties of Al2O3-C materials

Zou Xin, Xiao Xueping, Song Yanan, Chen Ping’an, Zhu Yingli, Li Xiangcheng   

  1. First author’s address:The State Key Laboratory of Refractories and Metallurgy,Wuhan University of Science and Technology,Wuhan 430081,Hubei,China
  • Received:2022-11-22 Online:2023-08-15 Published:2023-08-30

B4C添加量对Al2O3-C材料性能的影响

邹鑫1), 肖学平1), 宋雅楠1),2), 陈平安1), 朱颖丽1), 李享成1)   

  1. 1)武汉科技大学 省部共建耐火材料与冶金国家重点实验室 湖北武汉 430081
    2)浙江自立新材料股份有限公司 浙江绍兴 312369
  • 作者简介:邹鑫:男,1998年生,硕士研究生。 E-mail:2406313742@qq.com
  • 基金资助:
    湖北省重点研发项目(2020BAA028);湖北省创新群体项目(2020CFA038);国家自然科学基金项目(51972242和51774218)。

Abstract: Al2O3-C materials were prepared using tabular corundum (≤1 and ≤0.075 mm),Al-Si alloy powder (50 μm),α-Al2O3 micropowder (5 μm),flake graphite (≤0.074 mm) and B4C powder (20 μm) as raw materials,nickel nitrate as the catalyst,and phenolic resin as the binder.Effects of B4C additions (0,3%,6% and 9%,by mass) on the properties of Al2O3-C materials were investigated.The results show that:(1)with the increase of the B4C addition,the linear change rate of the specimens decreases obviously,the cold modulus of rupture and the cold compressive strength increase significantly; with 3% B4C,the linear change rate of the specimen after treatment at 1 450 ℃ decreases to 0.65%,the cold modulus of rupture and the cold compressive strength increase to the maximum values of 28.7 and 57.3 MPa,respectively;(2)with 6% B4C,the oxidation index of the specimen oxidized at 1 400 ℃ in air atmosphere decreases to a minimum of 3.9%,showing significantly enhanced oxidation resistance.

Key words: alumina-carbon, boron carbide, mechanical properties, oxidation resistance

摘要: 以板状刚玉(粒度≤1、≤0.075 mm)、Al-Si合金粉(粒度为50 μm)、α-Al2O3微粉(粒度为5 μm)、鳞片石墨(粒度≤0.074 mm)和B4C粉(粒度为20 μm)为原料,硝酸镍为催化剂,酚醛树脂为结合剂制备了Al2O3-C材料,研究了B4C添加量(加入质量分数分别为0、3%、6%和9%)对Al2O3-C材料性能的影响。结果表明:1)随着B4C添加量的增加,试样的线变化率明显减小,常温抗折强度和耐压强度明显增大;当B4C添加量为3%(w)时,试样经1 450 ℃处理后的线变化率降至0.65%,常温抗折强度和耐压强度最高,分别为28.7和57.3 MPa。2)当B4C添加量为6%(w)时,试样经1 400 ℃空气气氛氧化后的氧化指数降至3.9%,抗氧化能力明显增强。

关键词: Al2O3-C, B4C, 力学性能, 抗氧化性能