Refractories ›› 2025, Vol. 59 ›› Issue (4): 283-288.DOI: 10.3969/j.issn.1001-1935.2025.04.002

Previous Articles     Next Articles

Effects of chopped glass fibers on properties of silica sol bonded corundum castables

Ding Yuhang, Liu Hui-yong, Wei Jianxiu, Xiong Jiquan, Xiang Bing, Xia Changyong   

  1. First author's address:Wuhan Research Institute of Metallurgy Construction Co.,Ltd.of MCC Group,Wuhan 430081,Hubei,China
  • Received:2024-11-06 Published:2025-08-18

短切玻璃纤维对硅溶胶结合刚玉质浇注料性能的影响

丁宇航, 刘会永, 魏建修, 熊继全, 项冰, 夏昌勇   

  1. 中冶武汉冶金建筑研究院有限公司 湖北武汉 430081
  • 作者简介:丁宇航:男,1995年生,硕士,工程师。E-mail:2448328299@qq.com
  • 基金资助:
    国家重点研发计划(2018YFB1502903)。

Abstract: Improving the green body mechanical strength and thermal shock resistance of silica sol bonded corundum castables is of great significance for promoting their large-scale application.Silica sol bonded corundum castables were prepared with brown corundum,dense corundum powder,α-Al2O3 micropowder and SiO2 micropowder as the main raw materials,and silica sol as the binder.The effects of different extra-additions of chopped glass fibers (0,0.2%,0.4%,0.6%,0.8% and 1%,by mass) on the properties of the castables were studied.The results show that with the increase of the fiber addition,the cold modulus of rupture,cold compressive strength and hot modulus of rupture of the samples first increase and then decrease.After drying at 110 ℃,the sample containing 0.4% fibers has the cold modulus of rupture of 9.1 MPa and cold compressive strength of 27.4 MPa,increasing by 80.4% and 41.2%,respectively,compared with the one without fibers.This is because the fibers combine with the silica sol gel interface to form a stressed skeleton,strengthening the bonding between the matrix and the aggregates.When subjected to external stress,the fibers can effectively share the load and prevent crack propagation,thus increasing the strength.In addition,the sample with 0.4% fibers has the highest cold modulus of rupture before and after thermal shock,and its strength retention ratio increases by 16.1% compared to the sample without fibers.Generally,the sample with 0.4% fibers exhibits the best comprehensive performance.

Key words: corundum castables, silica sol, glass fibers, mechanical properties

摘要: 提高硅溶胶结合刚玉质浇注料生坯的机械强度和抗热震性能对于促进其大规模应用具有重要意义。以棕刚玉、致密刚玉粉、α-Al2O3微粉、SiO2微粉为主要原料,硅溶胶为结合剂,制备硅溶胶结合刚玉质浇注料。研究了不同短切玻璃纤维外加量(外加质量分数分别为0、0.2%、0.4%、0.6%、0.8%、1%)对该浇注料性能的影响。结果表明:随着纤维外加量的增加,试样的常温抗折强度、常温耐压强度和高温抗折强度先增大后减小,110 ℃干燥后,外加0.4%(w)纤维试样的常温抗折与耐压强度达到9.1和27.4 MPa,相比于未添加纤维的试样分别提高了80.4%和41.2%,这是由于加入的纤维与硅溶胶凝胶界面结合形成了受力骨架,强化了基质与骨料的连接;同时,在受到外加应力时,纤维可以有效地分担载荷并阻止裂纹的扩展,使强度提高。此外,外加 0.4%(w)纤维的试样热震前后常温抗折强度最高,抗折强度保持率相比于未加入纤维的试样提升了16.1%。综上,外加0.4%(w)纤维试样的综合性能最佳。

关键词: 刚玉质浇注料, 硅溶胶, 玻璃纤维, 力学性能