Refractories ›› 2026, Vol. 60 ›› Issue (2): 93-97.DOI: 10.3969/j.issn.1001-1935.2026.02.001

    Next Articles

Preparation of SiC ceramic by reactive melt infiltration and their impact resistance

Sun Mengyong, Qu Junfeng, Li Guobin, Wang Wenlong, Sun Shuli, Feng Ying   

  1. First author’s address:52nd Research Institute,China North Industries Group Corporation Limited,Yantai 264003,Shandong,China
  • Received:2025-04-29 Online:2026-04-15 Published:2026-04-15

反应熔融渗透法制备SiC陶瓷及其抗冲击性能研究

孙孟勇, 曲俊峰, 李国斌, 王雯龙, 孙淑丽, 冯莹   

  1. 中国兵器工业集团第五二研究所 山东烟台 264003
  • 作者简介:孙孟勇:男,1990年生,博士,副研究员。E-mail:sunmy@mail.nwpu.edu.cn

Abstract: To reveal the dynamic damage mechanism of SiC ceramics,a SiC ceramic was fabricated via reactive melt infiltration using SiC powder,B4C powder and carbon powder as starting materials,and Si powder as the infiltrant.The phase composition,microstructure and impact resistance of the as-prepared ceramic were mainly investigated,and the dynamic mechanical behavior was analyzed.The results show that the SiC ceramic contains SiC,B12(C,Si,B)3 and Si;and the residual silicon content is 14.3%-15% by volume.The ceramic exhibits flexural strength of 340 MPa,fracture toughness of 4.6 MPa·m1/2,and Vickers hardness of 20.5 GPa.The ceramic presents an obvious single-peak strain rate strengthening effect;when the true stress reaches 1 950 MPa,cracks propagate preferentially along the impact loading direction,and the material undergoes avalanche crushing after damage accumulates to a critical point.

Key words: silicon carbide ceramics, reactive melt infiltration, impact resistance, dynamic damage

摘要: 为了揭示SiC陶瓷的动态损伤机制,以SiC粉、B4C粉、炭粉为原料,以Si粉为熔渗剂,采用反应熔融渗透法制备了SiC陶瓷,主要研究了材料的物相组成、显微形貌和抗冲击性能,并对其动态行为进行了分析。结果表明:制备的SiC陶瓷残余硅含量为14.3%~15%(φ),物相包括SiC、B12(C,Si,B)3及Si,材料的弯曲强度为340 MPa,断裂韧性为4.6 MPa·m1/2,维氏硬度达20.5 GPa;陶瓷表现出显著的单峰应变率强化效应,真应力最大值为1 950 MPa时,裂纹沿冲击加载方向优先扩展,损伤累积至临界点后材料发生雪崩式粉碎。

关键词: 碳化硅陶瓷, 反应熔融渗透法, 抗冲击性能, 动态损伤

CLC Number: