Refractories ›› 2022, Vol. 56 ›› Issue (1): 75-81.DOI: 10.3969/j.issn.1001-1935.2022.01.017
Previous Articles Next Articles
Dong Bo(
), Yu Chao, Deng Chengji(
), Zhu Hongxi, Ding Jun, Zhu Qingyou
Received:2021-06-10
Online:2022-02-15
Published:2022-02-24
Contact:
Deng Chengji
通讯作者:
邓承继
作者简介:董博:男,1992年生,博士研究生。E-mail: dongbo1105@163.com
基金资助:CLC Number:
Dong Bo, Yu Chao, Deng Chengji, Zhu Hongxi, Ding Jun, Zhu Qingyou. Research progress on hot performance of reaction sintered silicon carbide[J]. Refractories, 2022, 56(1): 75-81.
董博, 余超, 邓承继, 祝洪喜, 丁军, 朱青友. 反应烧结碳化硅高温性能的研究进展[J]. 耐火材料, 2022, 56(1): 75-81.
Add to citation manager EndNote|Ris|BibTeX
URL: http://www.nhcl.cn/EN/10.3969/j.issn.1001-1935.2022.01.017
| [1] | 昝文宇, 马北越. 高纯SiC微粉制备进展[J]. 耐火材料, 2021,55(2):161-168. |
| [2] | 李辰冉, 谢志鹏, 康国兴, 等. 国内外碳化硅陶瓷材料研究与应用进展[J]. 硅酸盐通报, 2020,39(5):1353-1370. |
| [3] | 郝寅雷, 赵文兴, 翁志成. 新型反射镜材料——碳化硅[J].宇航材料工艺, 2001,31(4):11-14+53. |
| [4] | 盛况, 郭清, 张军明, 等. 碳化硅电力电子器件在电力系统的应用展望[J].中国电机工程学报, 2012, 32(30):1-7+3. |
| [5] | 张勇, 何新波, 曲选辉, 等. 碳化硅陶瓷的放电等离子烧结[J]. 北京科技大学学报, 2008,30(12):1414-1417. |
| [6] | ŠAJGALÍK P, SEDLÁCEK J, LENCÉŠ Z, et al. Additive-free hot-pressed silicon carbide ceramics—A material with exceptional mechanical properties[J]. Journal of the European Ceramic Society, 2016,36(6):1333-1341. |
| [7] | 佘继红, 江东亮, 谭寿洪, 等. 碳化硅陶瓷的热等静压烧结[J]. 硅酸盐学报, 1997,25(4):395-400. |
| [8] | LI Y S, YIN J, WU H B, et al. High thermal conductivity in pressureless densified SiC ceramics with ultra-low contents of additives derived from novel boron-carbon sources[J]. Journal of the European Ceramic Society, 2014,34(10):2591-2595. |
| [9] | 王艳香, 谭寿洪, 江东亮. 反应烧结碳化硅的研究与进展[J]. 无机材料学报, 2004,19(3):456-462. |
| [10] | 艾俊迪, 余超, 董博, 等. 添加Al粉对反应烧结碳化硅性能和结构的影响[J]. 耐火材料, 2021,55(1):51-55. |
| [11] | SONG N, ZHANG H B, LIU H,et al. Effects of SiC whiskers on the mechanical properties and microstructure of SiC ceramics by reactive sintering[J]. Ceramics International, 2017,43(9):6786-6790. |
| [12] | HAYUN S, FRAGE N, DARIEL M P. The morphology of ceramic phases in BxC-SiC-Si infiltrated composites[J]. Journal of Solid State Chemistry, 2006,179(9):2875-2879. |
| [13] | LI S, ZHANG Y M, HAN J C,et al. Random chopped fibers in reaction bonded SiC composite:Morphology,etching and reinforcing properties[J]. Materials Science and Engineering A, 2012,551:104-109. |
| [14] | CHAKRABARTI O P, DAS P K. High temperature load-deflection behaviour of reaction bonded SiC (RBSC)[J]. Ceramics International, 2001,27(5):559-563. |
| [15] | LIU W, CHENG L F, WANG Y G,et al. Investigation of the residual stress in reaction-bonded SiC under irradiation[J]. Journal of the European Ceramic Society, 2016,36(16):3901-3907. |
| [16] | HUANG Q W, ZHU L H. High-temperature strength and toughness behaviors for reaction-bonded SiC ceramics below 1 400 ℃[J]. Materials Letters, 2005,59(14-15):1732-1735. |
| [17] | RAO X S, ZHANG F H, LUO X C,et al. Characterization of hardness,elastic modulus and fracture toughness of RB-SiC ceramics at elevated temperature by Vickers test[J]. Materials Science and Engineering A, 2019,744:426-435. |
| [18] | HUANG Q W, JIN Z H. The high temperature oxidation behavior of reaction-bonded silicon carbide[J]. Journal of Materials Processing Technology, 2001,110(2):142-145. |
| [19] | KIM H W, KIM H E, SONG H,et al. Effect of oxidation on the room-temperature flexural strength of reaction-bonded silicon carbides[J]. Journal of the American Ceramic Society, 1999,82(6):1601-1604. |
| [20] | SHAN Q L, HU J B, YANG J S,et al. Oxidation behavior of Al2O3 added reaction-sintered SiC ceramics in wet oxygen environment at 1 300 ℃[J]. Journal of Asian Ceramic Societies, 2018,6(3):254-261. |
| [21] | LIM C B, YANO T, ISEKI T. Microstructure and mechanical properties of RB-SiC/MoSi2 composite[J]. Journal of Materials Science, 1989,24(11):4144-4151. |
| [22] | SLACK G A. Thermal conductivity of pure and impure silicon,silicon carbide,and diamond[J]. Journal of Applied Physics, 1965,35(12):3460-3466. |
| [23] | NAKANO H, WATARI K, KINEMUCHI Y,et al. Microstructural characterization of high-thermal-conductivity SiC ceramics[J]. Journal of the European Ceramic Society, 2004,24(14):3685-3690. |
| [24] | 李其松. 高热导率SiC陶瓷材料制备及应用研究[D]. 济南:山东大学, 2016. |
| [25] | ZHANG Y Y, HSU C Y, AUBUCHON S,et al. Microstructural and thermal property evolution of reaction bonded silicon carbide (RBSC)[J]. Journal of Alloys and Compounds, 2018,764:107-111. |
| [26] | 雷海波. 再结晶碳化硅陶瓷抗氧化及抗热震性能研究[D]. 长沙:湖南大学, 2010. |
| [27] | HASSELMAN D P H. Grifjfith criterion and thermal shock resistance of single-phase versus multiphase brittle ceramics[J].Journal of the American Ceramic Society,l969, 52(5):288-289. |
| [28] | 朱丽慧, 黄清伟. 反应烧结碳化硅材料的抗热震性能研究[J]. 耐火材料, 2001,35(4):202-204. |
| [29] | 李连跃, 孙洪鸣, 田素贵, 等. 炭黑含量对反应烧结碳化硅组织与性能的影响[J]. 中国陶瓷工业, 2017,24(1):18-22. |
| [30] | SONG S C, LU B H, GAO Z Q,et al. Microstructural development and factors affecting the performance of a reaction-bonded silicon carbide composite[J]. Ceramics International, 2019,45(14):17987-17995. |
| [31] | SUYAMA S, KAMEDA T, ITOH Y. Development of high-strength reaction-sintered silicon carbide[J]. Diamond and Related Materials, 2003,12(3-7):1201-1204. |
| [32] | 杨新领, 郑奔, 李志强, 等. 碳化硅粒度对反应烧结碳化硅陶瓷显微结构与性能的影响[J]. 科技创新导报, 2016,13(2):29-31. |
| [33] | 刘开松. 凝胶注模成型制备反应烧结碳化硅性能的研究[D]. 武汉:武汉理工大学, 2011. |
| [34] | 邓明进, 武七德, 吉晓莉, 等. 酚醛树脂对反应烧结碳化硅显微结构与性能的影响[J]. 耐火材料, 2008,42(4):267-270. |
| [35] | 付旻慧, 刘凯, 刘洁, 等. 碳化硅零件的激光选区烧结及反应烧结工艺[J]. 中国机械工程, 2018,29(17):2111-2118. |
| [36] | MEYERS S, LEERSNIJDER L D, VLEUGELS J,et al. Direct laser sintering of reaction bonded silicon carbide with low residual silicon content[J]. Journal of the European Ceramic Society, 2018,38(11):3709-3717. |
| [37] | 杨新领, 章潇, 贾马龙, 等. 成型压力对反应烧结碳化硅显微结构与性能的影响[J].材料导报, 2015, 29(S2):536-537+567. |
| [38] | 崔聪聪, 张舸. 前驱体浸渍对反应烧结碳化硅性能的影响[C]// 2015光学精密工程论坛论文集,长春, 2015: 184-189. |
| [39] | GRINCHUK P S, KIYASHKO M V, ABUHIMD H M,et al. Effect of technological parameters on densification of reaction bonded Si/SiC ceramics[J]. Journal of the European Ceramic Society, 2018,38(15):4815-4823. |
| [40] | 巫红燕, 张国军, 王伟春. 烧结温度对反应烧结碳化硅组织与性能的影响[J]. 粉末冶金技术, 2017,35(5):342-346. |
| [41] | ZHANG N L, YANG J F, DENG Y C,et al. Preparation and properties of reaction bonded silicon carbide (RB-SiC) ceramics with high SiC percentage by two-step sintering using compound carbon sources[J]. Ceramics International, 2019,45(12):15715-15719. |
| [42] | 黄清伟, 高积强, 金志浩. 热处理温度对反应烧结碳化硅材料组织与性能的影响[J]. 耐火材料, 2000,34(1):17-19. |
| [43] | BERJONNEAU J, CHOLLON G, LANGLAIS F. Deposition process of Si-B-C ceramics from CH3SiCl3/BCl3/H2 precursor[J]. Thin Solid Films, 2008,516(10):2848-2857. |
| [44] | AROATI S, CAFRI M, DILMAN H,et al. Preparation of reaction bonded silicon carbide (RBSC) using boron carbide as an alternative source of carbon[J]. Journal of the European Ceramic Society, 2011,31(5):841-845. |
| [45] | HAN I S, LEE K S, SEO D W,et al. Improvement of mechanical properties in RBSC by boron carbide addition[J]. Journal of Materials Science Letters, 2002,21(9):703-706. |
| [46] | MUÑOZ A, FERNÁNDEZ J M, RODRÍGUEZ A D, et al. High-temperature compressive strength of reaction-formed silicon carbide (RFSC) ceramics[J]. Journal of the European Ceramic Society, 1998,18(1):65-68. |
| [47] | JUNG Y I, PARK D J, PARK J H,et al. Effect of TiSi2/Ti3SiC2 matrix phases in a reaction-bonded SiC on mechanical and high-temperature oxidation properties[J]. Journal of the European Ceramic Society, 2016,36(6):1343-1348. |
| [48] | 李可琢, 张海军, 苑高千, 等. 聚碳硅烷制备SiC陶瓷研究进展[J]. 耐火材料, 2020,54(3):260-265. |
| [49] | 王军凯, 邓先功, 张海军, 等. 碳纳米管增强碳复合耐火材料的研究进展[J].耐火材料, 2016, 50(2):150-154+157. |
| [50] | 曾凡, 陈建军, 姜敏, 等. SiC纳米线增强反应烧结碳化硅陶瓷的性能研究[J]. 硅酸盐通报, 2018,37(2):586-590. |
| [51] | XUE R, LIU P, ZHANG Z J,et al. Improvement of toughness of reaction bonded silicon carbide composites reinforced by surface-modified SiC whiskers[J]. Ceramics International, 2021,47(13):18150-18156. |
| [52] | SONG N, LIU H, FANG J Z. Fabrication and mechanical properties of multi-walled carbon nanotube reinforced reaction bonded silicon carbide composites[J]. Ceramics International, 2016,42(1):351-356. |
| [53] | 宋索成, 鲍崇高, 陈子晗, 等. 碳纤维改性反应烧结碳化硅陶瓷组织及力学性能[J]. 西安交通大学学报, 2017, 51(4):67-71+108. |
| [54] | ZHANG Y M, LI S, HAN J C,et al. Fabrication and characterization of random chopped fiber reinforced reaction bonded silicon carbide composite[J]. Ceramics International, 2012,38(2):1261-1266. |
| [55] | LI S, ZHANG Y M, HAN J C,et al. Effect of carbon particle and carbon fiber on the microstructure and mechanical properties of short fiber reinforced reaction bonded silicon carbide composite[J]. Journal of the European Ceramic Society, 2013,33(4):887-896. |
| [1] | Yao Luyan, Han Bingqiang, Zhang Jinhua, Ke Changming. Effect of Ti-Si-Fe alloy addition on structure and properties of Si3N4 bonded SiC refractories [J]. Refractories, 2024, 58(4): 277-283. |
| [2] | Ling Xiaxia, Xiang Yubo, Zheng Han, Wu Jiguang. Fabrication of reaction-bonded silicon carbide via phenolic/epoxy resin gelcasting [J]. Refractories, 2024, 58(4): 329-333. |
| [3] | Shao Rongdan, Ju Maoqi, Cheng Shui-ming, Xia Changyong, Li Xuzhi, Zhang Han, Shan Jiangbo. Effect of boron oxide on mechanical properties of Al2O3-SiC-C castables [J]. Refractories, 2024, 58(3): 230-233. |
| [4] | Ju Maoqi, Ma Xiaoyi, Cheng Shuiming, Xia Changyong, Wei Jianxiu, Zhang Xiaocun, Shan Jiangbo, Gao Dongsheng. Effects of spent iron trough castable addition on properties of Al2O3-SiC-C castables [J]. Refractories, 2024, 58(3): 238-241. |
| [5] | Meng Hongtao, Ma Longbin, Liu Xin. Effect of pre-oxidation on oxidation resistance of nitrides bonded silicon carbide materials for coke ovens [J]. Refractories, 2024, 58(3): 242-245. |
| [6] | Guan Yunhe, Zheng Lijun, Luo Xudong, Niu Shunan. Preparation and properties of porous silicon carbide ceramic materials from iron tailings [J]. Refractories, 2024, 58(3): 246-250. |
| [7] | Deng Chengji, He Feng, Liang Yiming, Li Ji, Gao Chao, Mu Meng. Influence of TiO2 addition on phase composition and properties of porous SiC ceramics [J]. Refractories, 2024, 58(2): 93-98. |
| [8] | Min Changsheng, Dong Bo, Yu Chao, Deng Chengji, Xing Guangchao, Ding Jun, Liu Hao, Zhu Hong-xi. Effects of particle gradation on microstructure and mechanical properties of recrystallized SiC honeycomb ceramics [J]. Refractories, 2024, 58(2): 127-131. |
| [9] | Liu Jingjing, Yue Weidong, Xiong Fei, Shan Yanfang. Preparation of silicon carbide based porous ceramics with network cell wall and their particulate matter capture [J]. Refractories, 2024, 58(2): 132-136. |
| [10] | Liang Baoqing, Zhang Zhifeng, Wang Quanxi, Shang Junli, Li Hongyu, Zhao Chenrui, Zhao Yue. Effects of SiC polymer precursor and Zn composite powders on properties of Al2O3-C unfired slide plate materials [J]. Refractories, 2024, 58(2): 137-142. |
| [11] | Ju Maoqi, Xiao Yangwu, Xia Changyong, Liang Yonghe, Cong Peiyuan, Wei Jianxiu, Cai Wei, Chen Jinfeng. Thermodynamic calculation and slag resistance analysis of Al2O3-SiC-C taphole clay during corrosion [J]. Refractories, 2024, 58(2): 143-147. |
| [12] | Wang Wenlong, Chen Gang, Wang Hongjie, Liu Kai. Research status of toughening SiC composite ceramics [J]. Refractories, 2024, 58(1): 87-92. |
| [13] | Chang Cheng, Lyu Chunjiang, Gong Jianfeng, Huang Yifei, Ma Zhaoyang, Liu Zhen. Effect of industrial carbon black addition on properties of multiphase bonded silicon carbide refractories [J]. Refractories, 2023, 57(5): 412-416. |
| [14] | Cao Huiyan, Wan Longgang, Wang Jianbo, Liu Yun, Zheng Han, Zhang Xinhua, Feng Yanbin, Wu Jiguang. Oxidation of recrystallized SiC in 1 000 ℃ saturated steam [J]. Refractories, 2023, 57(5): 423-426. |
| [15] | Zhang Xifei, Chen Ding, Luo Qiong, Gu Huazhi, Huang Ao, Fu Lyuping. Effect of carbon black and pore forming agent on properties of reaction sintered silicon carbide [J]. Refractories, 2023, 57(4): 320-323. |
| Viewed | ||||||
|
Full text |
|
|||||
|
Abstract |
|
|||||