Refractories ›› 2022, Vol. 56 ›› Issue (5): 423-426.DOI: 10.3969/j.issn.1001-1935.2022.05.012

Previous Articles     Next Articles

Influence of characteristics of reactive alumina micropowder on properties of alumina based castables

Tang Hai, Shi Yingheng, Yuan Wenjie   

  1. The State Key Laboratory of Refractories and Metallurgy,Wuhan University of Science and Technology,Wuhan 430081,Hubei,China
  • Received:2021-11-03 Online:2022-10-15 Published:2022-11-07

活性氧化铝微粉对刚玉质浇注料性能的影响

唐海1), 石颖恒1), 员文杰1,2)   

  1. 1)武汉科技大学 省部共建耐火材料与冶金国家重点实验室 湖北武汉 430081
    2)武汉科技大学 高温材料与炉衬技术国家地方联合工程研究中心 湖北武汉 430081
  • 通讯作者: 员文杰,男,1980年生,博士,教授。E-mail:yuanwenjie@wust.edu.cn
  • 作者简介:唐海:男,1993年生,博士研究生。E-mail:tanghaiwust@163.com
  • 基金资助:
    湖北省中央引导地方科技发展专项项目(2019ZYYD076)。

Abstract: Effect of three commercial reactive alumina micropowders on the properties of alumina based castables was researched using tabular alumina,reactive alumina micropowder and calcium aluminate cement as raw materials.The results indicate that:(1)the CA6 formation is influenced by the impurities content,the particle size and the specific surface area of alumina micropowder;(2)smaller alumina powders with narrow particle size distribution present better filling effect in the castables;therefore,samples incorporated with this kind of reactive alumina micropowder present dense microstructure and excellent mechanical properties;(3)the strength of fired castables is also correlated with the sinterability of reactive alumina micropowder;samples added reactive alumina micropowders with similar particle size but larger specific surface area present higher strength.

Key words: reactive alumina micropowder, particle size distribution, specific surface area, alumina based castables, strength

摘要: 以板状刚玉、活性氧化铝微粉、铝酸钙水泥为原料制备了刚玉质浇注料。研究了3种市售活性氧化铝微粉对刚玉质浇注料性能的影响。结果表明:1)氧化铝微粉杂质含量、粒度与比表面积的差异会影响CA6的生成量。2)粒度更小、分布更窄的微粉对浇注料的填充效果最佳,因而添加该微粉的试样烧后呈现更致密的显微结构与更优的力学性能。3)刚玉质浇注料的烧后强度也与活性氧化铝的烧结性能相关,添加粒度相近但比表面积更大的活性氧化铝微粉的试样具有更高的抗折强度。

关键词: 活性氧化铝微粉, 粒度分布, 比表面积, 刚玉质浇注料, 强度