Refractories ›› 2023, Vol. 57 ›› Issue (5): 369-376.DOI: 10.3969/j.issn.1001-1935.2023.05.001

    Next Articles

Advanced refractories innovation boosts China’s strategy implementation

Li Hongxia   

  1. First author's address: State Key Laboratory of Advanced Refractories,Sinosteel Luoyang Institute of Refractories Research Co.,Ltd.,Luoyang 471039,Henan,China
  • Received:2023-07-26 Online:2023-10-15 Published:2023-10-26

先进耐火材料创新助推国家战略实施

李红霞   

  1. 中钢集团洛阳耐火材料研究院有限公司 先进耐火材料国家重点实验室 河南洛阳 471039
  • 作者简介:李红霞:女,1965年生,博士,正高级工程师。E-mail:lihongx0622@126.com
  • 基金资助:
    国家自然科学基金(51932008;U21A2059);国家重点研发计划(2021YFB3701404)。

Abstract: Refractories,indispensable supporting materials for high temperature technology,are widely used in steel,nonferrous metals,environmental protection,aerospace and other fields.Based on the important fundamental raw material industry and strategic emerging industries,the requirements of China’s high-quality development,green and dual carbon target,and defense and security strategies for advanced refractories were analyzed,and the status of refractories was summarized.The opportunities and challenges of the refractories industry were discussed in the light of its own high-quality,green and low-carbon development.In the end,combined with the implementation of the China’s development strategy,the future development directions of advanced refractories were proposed:digitization and intelligence of research and development,reduction and structural functionalization,advanced refractories for green and low-carbon new technologies,and key technologies and standards for refractories green-low-carbonization and digital manufacturing.

Key words: advanced refractories, high temperature technology, national strategy, green and low-carbon

摘要: 耐火材料是高温技术不可或缺的支撑材料,在钢铁、有色、环保、航空航天等领域应用广泛。从重要基础原材料产业和战略新兴产业出发,解析了国家高质量发展、绿色双碳、国防安全等战略对先进耐火材料的需求,总结了耐火材料的现状,并结合耐火材料工业自身高质量绿色低碳发展,讨论了其面临的机遇与挑战,最后结合国家发展战略实施,提出了研发的数字化与智慧化、减量化与结构功能化、绿色低碳新技术用先进耐火材料、耐火材料绿色低碳化数字化制造关键技术与标准等先进耐火材料未来的发展方向。

关键词: 先进耐火材料, 高温技术, 国家战略, 绿色低碳