Refractories ›› 2024, Vol. 58 ›› Issue (2): 99-103.DOI: 10.3969/j.issn.1001-1935.2024.02.002

Previous Articles     Next Articles

Effects of zirconia and lanthana co-doping on properties of porous cordierite ceramics

Zhang Hui, Chai Qian, Zhang Hong, Wang Yixing, Hao Chenxi, Wang Xingyu   

  1. First author's address: Huaqing College,Xi'an University of Architecture and Technology,Xi'an 710043,Shaanxi,China
  • Received:2023-07-12 Online:2024-04-15 Published:2024-04-24

氧化锆和氧化镧共掺杂对堇青石多孔陶瓷性能的影响

张会, 柴倩, 张红, 王艺兴, 郝晨曦, 王星雨   

  1. 西安建筑科技大学 华清学院 陕西西安 710043
  • 作者简介:张会:女,1988年生,硕士,讲师。 E-mail:zhanghui26@126.com
  • 基金资助:
    陕西省教育厅专项科研计划项目(23JK0523);陕西省大学生创新创业训练计划项目创新训练项目(S202313679005)。

Abstract: To achieve the low temperature synthesis of cordierite,according to its theoretical ratio,porous cordierite ceramics were prepared using calcined kaolin (≤0.044 mm),sintered magnesia (≤0.074 mm) and silica micropowder (d50=2.6 μm) as main raw materials,analytically pure zirconia and lanthana as sintering aids,and polyvinyl alcohol (PVA) solution as the binder,pressing to samples of 30 mm×30 mm at 60 MPa,drying and calcining.The effects of the extra additions of zirconia (0 and 8%,by mass) and lanthana (0,0.2%,0.4%,0.6% and 0.8%,by mass) and calcination temperatures (1 200,1 250 and 1 300 ℃) on the cold physical properties,phase composition and microstructure of the porous cordierite ceramics were studied.The results show that:(1)the sample fired at 1 300 ℃ and introduced with 8% zirconia and 0.6% lanthana shows good physical properties;(2)the co-doping of zirconia and lanthana can improve the mechanical properties of the sample while maintaining the apparent porosity,and promote the formation of cordierite;(3)the co-doping of zirconia and lanthana can reduce the synthesis temperature of cordierite and improve the comprehensive performance of the sample.

Key words: cordierite, porous ceramics, sintering aid, zirconia, lanthana

摘要: 为实现堇青石相的低温合成,采用粒度为≤0.044 mm的煅烧高岭土、粒度为≤0.074 mm的烧结镁砂和d50=2.6 μm的二氧化硅微粉为主要原料,以分析纯的氧化锆和氧化镧为烧结助剂,以聚乙烯醇PVA溶液为结合剂,按照堇青石理论配比,在60 MPa压力下成型为 30 mm×30 mm的试样,干燥、煅烧后制备了堇青石多孔陶瓷。研究了烧结助剂氧化锆添加量(外加质量分数为0、8%)、氧化镧添加量(外加质量分数分别为0、0.2%、0.4%、0.6%、0.8%)和煅烧温度(分别为1 200、1 250及1 300 ℃)对堇青石多孔陶瓷常温物理性能、物相组成和显微结构的影响。结果表明:1)在1 300 ℃下,当试样中引入8%(w)氧化锆和0.6%(w)氧化镧时,试样的物理性能较优;2)氧化锆和氧化镧共掺杂可在显气孔率变化较小的情况下,提高试样的力学性能,且促进堇青石相的生成;3)氧化锆和氧化镧共掺杂可一定程度上降低堇青石相的合成温度,提高试样的综合性能。

关键词: 堇青石, 多孔陶瓷, 烧结助剂, 氧化锆, 氧化镧