Refractories ›› 2025, Vol. 59 ›› Issue (6): 477-481.DOI: 10.3969/j.issn.1001-1935.2025.06.004

Previous Articles     Next Articles

Effect of potassium feldspar addition on properties of ceramic proppant

Wang Chenzhe, Jin Endong, Ding Donghai, Xiao Guoqing, Zhu Xianfeng, Jia Xuhui   

  1. First author’s address:College of Materials Science and Engineering,Xi’an University of Architecture and Technology,Xi’an 710055,Shaanxi,China
  • Received:2025-03-12 Online:2025-12-15 Published:2025-12-23

钾长石添加量对陶粒支撑剂性能的影响

王晨喆1), 靳恩东1), 丁冬海1), 肖国庆1), 朱现峰2), 贾旭辉2)   

  1. 1)西安建筑科技大学 材料科学与工程学院 陕西西安 710055
    2)郑州市润宝耐火材料有限公司 河南郑州 452300
  • 作者简介:王晨喆:男,2000年生,硕士研究生。E-mail:wcz291457545@163.com
  • 基金资助:
    咸阳市重大科技创新专项(L2023-ZDKJ-QCY-SXGG-003)。

Abstract: To reduce the process cost and density of ceramic proppant,low-grade bauxite and coal gangue were adopted as raw materials,and potassium feldspar as sintering aid to prepare ceramic proppant.Green spherical pellets with particle sizes of 0.425-0.212 mm were obtained through granulation and sieving,then dried at 110 ℃ for 12 h and solid-phase-sintered at 1 220 ℃ for 2 h.The effects of the potassium feldspar addition (0,5%,10%,and 15%,by mass) on the density,breakage ratio,phase composition,and microstructure of the ceramic proppant were studied.The results show that (1)with the increase of the potassium feldspar addition,mullite and corundum crystals gradually grow and interlace with each other to form a reticulated structure,the liquid phase uniformly disperses and wraps the grains,enhancing the densification of the specimen;(2)during sintering,K2O in potassium feldspar forms a liquid phase with SiO2 and Al2O3,which fills the pores of the proppant and promotes the growth of corundum and mullite crystals,thereby reducing the breakage ratio and enhancing the mechanical strength;(3)when the potassium feldspar addition is 10%,the properties of the ceramic proppant are the optimal:bulk density of 1.41 g·cm-3,breakage ratio of 10.7% under a closure pressure of 35 MPa and 17.5% under 52 MPa.

Key words: ceramic proppant, potassium feldspar, mullite, breakage ratio

摘要: 为降低陶粒支撑剂工艺成本和密度,以低品位铝矾土和煤矸石为原料,钾长石为烧结助剂,通过造粒,筛分得到0.425~0.212 mm生坯球体,经110 ℃干燥12 h,再于1 220 ℃保温2 h固相烧结制备了陶粒支撑剂。研究钾长石添加量(质量分数分别为0、5%、10%、15%)对陶粒支撑剂的密度、破碎率、物相组成和显微结构的影响。结果表明:1)随着钾长石添加量的增加,莫来石和刚玉晶体逐渐长大,并互相交错形成网状结构,液相均匀分散并包裹于晶粒外,使试样致密化程度提高。2)在煅烧过程中,钾长石中的K2O与SiO2和Al2O3形成液相,填充了支撑剂的孔隙,并促进了刚玉和莫来石晶体的生长,从而降低破碎率,提高力学强度。3)当钾长石添加量为10%(w)时,陶粒支撑剂的性能达到最佳,其体积密度为1.41 g·cm-3,35 MPa闭合压力下破碎率为10.7%,52 MPa闭合压力下破碎率为17.5%。

关键词: 陶粒支撑剂, 钾长石, 莫来石, 破碎率

CLC Number: