Refractories ›› 2024, Vol. 58 ›› Issue (2): 174-178.DOI: 10.3969/j.issn.1001-1935.2024.02.015

Previous Articles     Next Articles

Research progress on preparation of mullite materials from industrial solid wastes

Sun Jiaqu, Liu Xin, Wu Feng, He Huiling, Luo Xudong   

  1. First author's address: School of Materials and Metallurgy,University of Science and Technology Liaoning,Anshan 114051,Liaoning,China
  • Received:2023-07-03 Online:2024-04-15 Published:2024-04-24

工业固废制备莫来石材料的研究进展

孙家朐1), 刘新1), 吴锋1), 何慧龄1), 罗旭东1,2)   

  1. 1)辽宁科技大学 材料与冶金学院 辽宁鞍山 114051
    2)辽宁科技学院 辽宁本溪 117004
  • 作者简介:孙家朐:男,1999年生,硕士研究生。 E-mail:sunjj@ustl.edu.cn
  • 基金资助:
    国家自然科学基金资助项目(U20A20239);辽宁科技大学大学生创新创业训练项目。

Abstract: To solve the environmental pollution problem caused by the accumulation of bulk industrial solid wastes,the current research state on the preparation of mullite materials from industrial solid wastes was summarized.The preparation of mullite materials from alumina-rich and silica-rich industrial solid wastes was analyzed and summarized.The main problems encountered were pointed out,and the future development direction was looked forward.

Key words: industrial solid waste, mullite, coal ash, gangue

摘要: 为解决大宗工业固废堆积所造成的环境污染问题,概述了工业固废制备莫来石材料的研究现状,对富铝、富硅工业固废制备莫来石材料的研究进行了分析总结,指出目前工业固废制备莫来石材料面临的主要问题,并对其未来发展方向进行了展望。

关键词: 工业固废, 莫来石, 粉煤灰, 煤矸石