Refractories ›› 2026, Vol. 60 ›› Issue (2): 173-178.DOI: 10.3969/j.issn.1001-1935.2026.02.016

Previous Articles     Next Articles

Research progress on strengthening and toughening of high-alumina high-voltage electric porcelain materials

Yue Yonggang, Tian Xiaoyun, Dang Dawei, Li Zhihui, Jing Nan, Chong Xiaochuan, Ding Donghai, Xiao Guo-qing   

  1. First author’s address:Inner Mongolia Ultra High Voltage Power Supply Branch,Inner Mongolia Power Group,Hohhot 010080,Inner Mongolia
  • Received:2025-06-10 Online:2026-04-15 Published:2026-04-15

高铝质高压电瓷材料强韧化研究进展

岳永刚1), 田晓云1), 党大威1), 李智辉1), 景楠2), 种小川2), 丁冬海2), 肖国庆2)   

  1. 1)内蒙古电力(集团)有限责任公司 内蒙古超高压供电分公司 内蒙古呼和浩特 010080
    2)西安建筑科技大学 材料科学与工程学院 陕西西安 710055
  • 作者简介:岳永刚:男,1979年生,硕士,正高级工程师。E-mail:hvyue@163.com
  • 基金资助:
    2024年度科技项目(2024-4-30;2024-4-32)。

Abstract: Nowadays,high-alumina electric porcelain has become a core component to ensure the safe operation of the power grids.Due to its brittleness and high sensitivity to defects,traditional electric porcelain struggles to meet the reliability requirements for extreme environments,therefore,the research and development of high-strength and high-toughness high-voltage electric porcelain has become the key to ensuring the long-term stable operation of the power grids.Three effective methods for enhancing the performance of high-alumina high-voltage electric porcelain materials and their mechanisms were summarized:the optimization of the preparation process improves the mechanical properties and reliability through improving the densification and uniformity of the materials;the optimization of raw material selection,which adjusts the ratio and improves the purity,enhances the mechanical strength and electrical insulation;and additive toughening technology,especially whisker toughening and nanoparticle dispersion toughening,significantly improves the fracture toughness and resistance to crack propagation.

Key words: high-voltage electric porcelain, high-alumina, strengthening and toughening, fracture toughness, electrical insulation

摘要: 目前,高铝质电瓷已成为保障电网安全运行的核心部件。传统电瓷因脆性大、缺陷敏感性高,难以适应极端环境的可靠性需求,故高强韧高压电瓷的研发成为保障电网长期稳定运行的关键。综述了提升高铝质高压电瓷材料性能的3类有效方法及其作用:制备工艺优化通过提高材料致密性与均匀性,改善力学性能和可靠性;原料选择优化借助调整配比与提升纯度,增强机械强度和电绝缘性;添加剂增韧技术(尤其晶须增韧和纳米颗粒弥散增韧),可显著提高断裂韧性和抗裂纹扩展能力。

关键词: 高压电瓷, 高铝, 强韧化, 断裂韧性, 电绝缘性