Refractories ›› 2022, Vol. 56 ›› Issue (6): 523-526.DOI: 10.3969/j.issn.1001-1935.2022.06.014

Previous Articles     Next Articles

Wettability of silica sol modified multilayer graphene

Yu Baisong, Zhu Yening, Li Yangzhe, Su Yuqing, Wei Juncong, Tu Junbo, Wang Yilong   

  1. Hebei Province Key Laboratory of Inorganic Nonmetallic Materials,North China University of Science and Technology,Tangshan 063210,Hebei,China
  • Received:2021-12-22 Online:2022-12-15 Published:2022-12-26

硅溶胶改性多层石墨烯的润湿性研究

郁柏松1), 朱业宁1), 李炀哲1), 苏玉庆1), 魏军从1), 涂军波1), 王义龙2)   

  1. 1)华北理工大学 河北省无机非金属材料重点实验室 河北唐山 063210
    2)唐山市国亮特殊耐火材料有限公司 河北唐山 063000
  • 通讯作者: 涂军波,男,1971年生,博士,教授。E-mail:tujunbo@126.com
  • 作者简介:郁柏松:男,1995年生,硕士研究生。E-mail:994575303@qq.com
  • 基金资助:
    河北省自然科学基金资助项目(E2017209164)。

Abstract: To expand the application of multilayer graphene in water-based systems,modified multilayer graphene was prepared by vacuum impregnation with silica sol and carbon-embedded heat treatment at 300,500 or 700 ℃ for 3 h.The phase composition,the microstructure and the wettability of the modified multilayer graphene heat treated at different temperatures were studied.The results show that the water wettability of the modified multilayer graphene is improved after vacuum impregnation with silica sol and carbon-embedded heat treatment;the optimum heat treatment temperature is 300 ℃,and the modified multilayer graphene has the water wetting angle of 64.7°.

Key words: multilayer graphene, surface modification, silica sol, vacuum impregnation method, wetting angle

摘要: 为扩展多层石墨烯在水基体系中的应用,采用硅溶胶真空浸渍并在埋碳气氛下分别于300、500、700 ℃保温3 h,制备得到改性多层石墨烯。研究了不同热处理温度下改性石墨烯的物相组成、显微结构和润湿性。结果表明:经硅溶胶真空浸渍及埋碳热处理后,改性多层石墨烯润湿性提高;最佳热处理温度为300 ℃,热处理后改性多层石墨烯的润湿角为64.7°。

关键词: 多层石墨烯, 表面改性, 硅溶胶, 真空浸渍法, 润湿角

CLC Number: