Refractories ›› 2025, Vol. 59 ›› Issue (1): 65-69.DOI: 10.3969/j.issn.1001-1935.2025.01.012

Previous Articles     Next Articles

Effect of process parameters on oxidation resistance and hydration resistance of Al2O3-C refractories

Zhang Rui, Sun Xudong, Wei Han, Yuan Biao, Wang Juntao, Yuan Lin, Liu Shifan, Chen Songlin   

  1. First author’s address:Ruitai Materials Technology Co.,Ltd.,China Building Materials Academy Co.,Ltd.,Beijing 100024,China
  • Received:2024-05-20 Online:2025-02-15 Published:2025-02-27

工艺参数对Al2O3-C耐火材料抗氧化性和抗水化性的影响

张瑞1), 孙旭东1), 魏瀚1), 袁彪2,3), 王俊涛1)袁林1), 刘士范2,3), 陈松林1,3)   

  1. 1)中国建筑材料科学研究总院瑞泰科技股份有限公司 北京 100024
    2)宜兴市耐火材料有限公司 江苏宜兴 214265
    3)江苏省节能环保型冶金用高温耐火材料工程技术研究中心 江苏宜兴 214265
  • 通讯作者: 陈松林,男,1976年生,博士,教授。E-mail:chensonglinc@126.com
  • 作者简介:* 张瑞:男,1998年生,硕士。E-mail:2499507427@qq.com

Abstract: To optimize the preparation process of Al2O3-C refractories,the influence of various factors on the oxidation resistance and hydration resistance of the refractories was studied.Cylindrical samples of 50 mm×50 mm were prepared using tabular corundum,Al powder,fused zirconia corundum,activated alumina powder and graphite as the main raw materials and thermosetting phenolic resin as the binder,hydro-forming and heat treating in a carbon embedded atmosphere.The Al powder addition (6%,9% and 12%,by mass),graphite addition (5%,15% and 25%,by mass),heat treatment temperature (680,950 and 1 500 ℃) and thermal insulating time (3,6 and 9 h) were selected as the research factors,and three levels of each factor were selected for orthogonal design.The results show that:(1)the additions of Al powder and graphite are the main factors affecting the oxidation resistance,while the heat treatment temperature and thermal insulating time are the secondary factors;(2)the Al powder addition and heat treatment temperature are the main factors affecting the hydration resistance,while the graphite addition and thermal insulating time are the secondary factors;(3)comprehensively considering,the optimal process is 9% Al powder,5% graphite,heat treatment temperature of 1 500 ℃ and thermal insulating time of 6 h,and the prepared sample contains columnar Al4O4C,which can significantly improve the oxidation resistance and hydration resistance of the materials.

Key words: Al2O3-C refractories, Al4O4C, hydration resistance, oxidation resistance

摘要: 为了研究各因素对Al2O3-C耐火材料抗氧化和抗水化性能的影响,以优化其制备工艺,以板状刚玉、Al粉、电熔锆刚玉、活性氧化铝粉、鳞片石墨为主要原料,使用热固性酚醛树脂为结合剂,采用液压成型制成 50 mm×50 mm 的圆柱体试样,在埋碳气氛下对试样进行了热处理。选取Al粉加入量(加入质量分数分别为6%、9%和12%)、石墨加入量(加入质量分数分别为5%、15%和25%)、热处理温度(680、950、1 500 ℃)和保温时间(3、6、9 h)为研究因素,每个因素选取3个水平进行正交设计,分析了其对Al2O3-C耐火材料抗氧化和抗水化性能的影响。结果表明:1)Al粉加入量和石墨加入量为影响抗氧化性能的主要因素,而热处理温度和保温时间为次要因素;2)Al粉加入量和热处理温度是影响抗水化性能的主要因素,而石墨加入量和保温时间为次要因素;3)综合考虑,最优工艺为:Al粉加入量9%(w),石墨加入量5%(w),热处理温度1 500 ℃,保温时间 6 h,制备的试样中存在柱状的Al4O4C,能够显著提高材料的抗氧化和抗水化性能。

关键词: Al2O3-C耐火材料, Al4O4C, 抗水化性能, 抗氧化性能