耐火材料 ›› 2026, Vol. 60 ›› Issue (1): 48-53.DOI: 10.3969/j.issn.1001-1935.2026.01.009

• 研究开发 • 上一篇    下一篇

隔热碳纤维复合材料微纳孔调控及其性能

陈嘉良, 丁军, 罗益欣, 刘正龙, 余超, 朱青友, 邓承继   

  1. 武汉科技大学 先进耐火材料全国重点实验室 湖北武汉 430081
  • 收稿日期:2025-03-24 出版日期:2026-02-15 发布日期:2026-02-26
  • 通讯作者: 朱青友,男,1986年生,实验师。E-mail:zhuqingyou@wust.edu.cn
  • 作者简介:陈嘉良:男,2000年生,硕士研究生。E-mail:1290248314@qq.com
  • 基金资助:
    *湖北省自然科学基金项目(2023BAB106);国家自然科学基金项目(52402034);武汉市自然科学基金项目(2024040701010051);湖北省科技创新团队基金项目(T2023001)。

Micro-nano pore control and properties of thermal insulation carbon fiber composites

Chen Jialiang, Ding Jun, Luo Yixin, Liu Zhenglong, Yu Chao, Zhu Qingyou, Deng Chengji   

  1. First author’s address: State Key Laboratory of Advanced Refractories,Wuhan University of Science and Technology,Wuhan 430081,Hubei,China
  • Received:2025-03-24 Online:2026-02-15 Published:2026-02-26

摘要: 为实现碳纤维复合材料的高效隔热,以T300碳纤维预浸布为增强体,环氧树脂为基体,通过溶剂诱导相分离策略构建多孔结构体系。采用异丙醇作为造孔剂,通过调控异丙醇的添加量(质量分数分别为0、10%、20%和30%)实现碳纤维复合材料孔隙率的梯度化设计,探究孔隙结构演化对材料力学与隔热性能的耦合作用机制。结果表明:随着异丙醇添加量从0增加至30%(w),复合材料孔隙率从0.71%提升至 2.14%,孔隙数量递增且孔隙尺寸扩增,孔隙形貌由点状缺陷转变为圆形缺陷,但力学性能呈现可控性衰减趋势;随着异丙醇添加量从0增加至30%(w),材料的隔热性能呈现逐渐上升的趋势;当异丙醇添加量为10%(w)时,材料的孔隙率为1.12%,材料的力学性能降低程度最小,且隔热性能相对最佳。

关键词: 碳纤维复合材料, 显微结构, 力学性能, 隔热性能

Abstract: To achieve efficient thermal insulation of carbon fiber composites,a porous structure system was constructed through the solvent-induced phase separation strategy using T300 carbon fiber prepregs as the reinforcement and epoxy resin as the matrix.Isopropyl alcohol was used as the pore-forming agent and the gradient design of the porosity in the carbon fiber composites was achieved by regulating its additions (0,10%,20% and 30%,by mass).The coupling mechanism of the pore structure evolution on the mechanical and thermal insulation properties of the materials was explored.The results show that:as the isopropyl alcohol addition increases from 0 to 30%,the porosity of the composites increases from 0.71% to 2.14%,accompanied by an increase in the pore number and size,the pore morphology evolves from point-like defects to circular defects,while the mechanical properties show a controllable degradation trend;meanwhile,the thermal insulation performance shows a gradually increasing trend.When the isopropyl alcohol addition is 10%,the material exhibits a porosity of 1.12%,achieving the minimal reduction in the mechanical properties and relatively optimal thermal insulation performance.

Key words: carbon fiber composites, microstructure, mechanical properties, thermal insulation performance

中图分类号: