耐火材料 ›› 2023, Vol. 57 ›› Issue (4): 347-350.DOI: 10.3969/j.issn.1001-1935.2023.04.015

• 生产应用 • 上一篇    下一篇

CaO添加量对中频炉用铝镁质干式捣打料性能的影响

胡燈1), 张寒1), 黄学忠2), 刘红波3), 赵惠忠1)   

  1. 1)武汉科技大学 省部共建耐火材料与冶金国家重点实验室 湖北武汉 430081
    2)广西北港新材料有限公司 广西北海 536000
    3)山东圣川新材料科技股份有限公司 山东淄博 255000
  • 收稿日期:2022-09-19 出版日期:2023-08-15 发布日期:2023-08-30
  • 通讯作者: 张寒,男,1985年生,博士,副教授。E-mail:wustzh@163.com
  • 作者简介:胡燈:男,1998年生,硕士研究生。E-mail:609964387@qq.com

Effect of CaO addition on properties of alumina-magnesia dry ramming mix for medium frequency furnaces

Hu Deng, Zhang Han, Huang Xuezhong, Liu Hongbo, Zhao Huizhong   

  1. First author’s address:The State Key Laboratory of Refractories and Metallurgy,Wuhan University of Science and Technology,Wuhan 430081,Hubei,China
  • Received:2022-09-19 Online:2023-08-15 Published:2023-08-30

摘要: 为提高中频感应炉的使用寿命,以电熔刚玉、电熔镁砂为主要原料,CaO为烧结添加剂,采用捣打成型的方式制备了铝镁质干式捣打料。研究CaO添加量(加入质量分数分别为0、0.5%、1%、1.5%、2%)对铝镁质干式捣打料经1 600 ℃热处理3 h后的物相组成、烧结性能及显微结构的影响。结果表明:适量的CaO能促进铝镁质干式捣打料的烧结,常温耐压强度得到了明显的改善,其原因在于CaO与Al2O3反应生成六铝酸钙(CA6),CA6穿插于刚玉相与尖晶石相之间,提高了捣打料的强度;当CaO添加量为1%(w)时,经1 600 ℃热处理后的捣打料综合性能最好,其线膨胀率为1.38%,体积密度为2.86 g·cm-3,显气孔率为21.3%,常温耐压强度为15.2 MPa。

关键词: 中频炉, 铝镁质干式捣打料, 烧结性能, 耐压强度

Abstract: In order to improve the service life of medium frequency furnaces,the alumina-magnesia dry ramming mix was prepared using fused corundum and fused magnesia as main raw materials and CaO as the sintering additive.The effects of the CaO addition (0,0.5%,1%,1.5%,and 2%,by mass) on the phase composition,sintering properties and microstructure of the ramming mix after heat treatment at 1 600 ℃ for 3 h were studied.The results show that an appropriate amount of CaO can promote the sintering of the alumina-magnesia dry ramming mix,and the cold compressive strength is significantly improved.The reason is that CaO reacts with Al2O3 to form hexaluminate (CA6),interposing between corundum and spinel.When the CaO addition is 1%,the ramming mix after heat treatment at 1 600 ℃ has the best comprehensive properties,with the linear expansion rate of 1.38%,bulk density of 2.86 g·cm-3,apparent porosity of 21.3% and cold compressive strength of 15.2 MPa.

Key words: medium frequency furnace, alumina-magnesia dry ramming mix, sintering properties, compressive strength