Refractories ›› 2021, Vol. 55 ›› Issue (6): 549-552.DOI: 10.3969/j.issn.1001-1935.2021.06.020

Previous Articles    

Research progress on performance optimization of porous mullite

Wang Lulu1,2)(), Ma Beiyue2)(), Liu Chunming1), Tian Jialong2), Yu Jingkun2)   

  1. 1) School of Materials Science and Engineering,Northeastern University,Shenyang 110819,Liaoning,China
  • Received:2020-10-30 Online:2021-12-15 Published:2021-12-10
  • Contact: Ma Beiyue

多孔莫来石性能优化的研究进展

王露露1,2)(), 马北越2)(), 刘春明1), 田家龙2), 于景坤2)   

  1. 1)东北大学 材料科学与工程学院 辽宁沈阳 110819
    2)东北大学 冶金学院 辽宁沈阳 110819
  • 通讯作者: 马北越
  • 作者简介:王露露:女,1990年生,博士研究生。E-mail: wanglljy@126.com
  • 基金资助:
    国家自然科学基金项目资助(U1908223)

Abstract:

The influences of the raw materials and the elements doping on the properties of porous mullite ceramics were summarized.On this basis,the problems during the preparation and application of the porous mullite ceramics were pointed out,and the future development direction was prospected.

Key words: mullite, raw materials, doping, porous ceramics, research progress

摘要:

综述了多孔莫来石陶瓷的合成原料和元素掺杂对其性能的影响。在此基础上,指出了多孔莫来石陶瓷在制备和应用过程中存在的问题,并展望了多孔莫来石陶瓷的未来发展方向。