Refractories ›› 2022, Vol. 56 ›› Issue (5): 369-373.DOI: 10.3969/j.issn.1001-1935.2022.05.001

    Next Articles

Preparation of lightweight insulation materials from forsterite and fly ash cenesphere

Xie Zhe, Deng Chengji, Dong Bo, Ding Jun, Zhu Hongxi, Zhou Nian, Yu Chao   

  1. The State Key Laboratory of Refractories and Metallurgy,Wuhan University of Science and Technology,Wuhan 430081,Hubei,China
  • Received:2021-11-30 Online:2022-10-15 Published:2022-11-07

利用镁橄榄石和粉煤灰漂珠制备轻质隔热材料的研究

谢哲, 邓承继, 董博, 丁军, 祝洪喜, 周念, 余超   

  1. 武汉科技大学 省部共建耐火材料与冶金国家重点实验室 湖北武汉 430081
  • 通讯作者: 余超,男,1986年生,副教授。E-mail:chaoyu@wust.edu.cn
  • 作者简介:谢哲:男,1993年生,硕士研究生。E-mail:736537989@qq.com
  • 基金资助:
    国家自然科学基金联合基金项目(U20A20239);湖北省自然科学基金面上项目(2020CFB692)。

Abstract: In order to reduce the raw material cost and the sintering temperature,lightweight insulation materials were fabricated using forsterite and fly ash cenesphere as main raw materials,and borax as the texturizer,heat treating at 800 ℃ for 1 h.The influence of the borax addition (5%,10%,20% and 30%,by mass) on the phase composition,the microstructure,and the properties of the materials was studied.The results show that:(1)the main phases of the prepared lightweight insulation materials are forsterite,aluminum borate,mullite,and quartz;(2)when the borax addition is 20%,magnesium borate forms and the sample has good comprehensive properties,the true porosity of 58.6%,the bulk density of 1.08 g·cm-3,the thermal conductivity of 0.150 W·m-1·K-1,and the cold compressive strength of 7.62 MPa.

Key words: fly ash cenesphere, forsterite, lightweight insulation materials, thermal conductivity, cold compressive strength

摘要: 为降低原料成本和烧成温度,以镁橄榄石和粉煤灰漂珠为主要原料,硼砂为调质剂,经800 ℃保温1 h热处理制备轻质隔热材料。研究了硼砂加入量(质量分数分别为5%、10%、20%和30%)对材料的物相组成、显微结构和性能的影响。结果表明:1)轻质隔热材料的主物相为镁橄榄石、硼酸铝、莫来石和石英;2)当硼砂加入量为20%(w)时,试样中生成硼酸镁相,材料具有较好的综合性能,真气孔率为58.6%,体积密度为1.08 g·cm-3,热导率为0.150 W·m-1·K-1,常温耐压强度为7.62 MPa。

关键词: 粉煤灰漂珠, 镁橄榄石, 轻质隔热材料, 热导率, 常温耐压强度