Analysis and improvement of typical problems in RH furnace immersion tubes and circulation tubes

Wen Weixin, Liu Jianwei, Wu Jiyu, Ji Weiye, Li Shiliang   

  1. First author’s address:Shandong Iron and Steel Group Rizhao Co.,Ltd.,Rizhao 276800,Shandong,China
  • Received:2024-08-14 Online:2025-04-15 Published:2025-04-14

RH炉浸渍管与环流管典型问题分析与改进

温维新, 刘建伟, 吴计雨, 季伟烨, 李世良   

  1. 山东钢铁集团日照有限公司 山东日照 276800
  • 作者简介:温维新:男,1978年生,硕士,高级工程师。E-mail:56297578@qq.com

Abstract: To effectively improve the online service life of vacuum tanks,the typical problems during service of the immersion tubes and circulation tubes in RH furnaces of Shandong Iron and Steel Group Rizhao Co.,Ltd.were analyzed.Corresponding improvement measures were implemented for the problems such as abnormal corrosion at the lower part of the immersion tubes,deep ring trench between the immersion tubes and circulation tubes,and broken bricks between the circulation tubes and lower vessels,so as to reduce the abnormal downline of the vacuum tanks.The average life of vacuum tanks is increased from 115.6 heats to 133.7 heats.

Key words: RH furnace, immersion tube, circulation tube, corrosion

摘要: 为有效提升真空槽在线使用寿命,对山东钢铁集团日照有限公司RH炉浸渍管与环流管使用过程中的典型问题进行分析,针对浸渍管下部的异常侵蚀、浸渍管与环流管之间的深环沟、环流管与下部槽之间的断砖等问题制定相应改进措施,减少了真空槽异常下线情况,使得真空槽平均寿命由115.6炉提高到133.7炉。

关键词: RH炉, 浸渍管, 环流管, 侵蚀