Refractories ›› 2021, Vol. 55 ›› Issue (4): 348-353.DOI: 10.3969/j.issn.1001-1935.2021.04.017

Previous Articles     Next Articles

Research progress of MgAlON and its composite materials

Xia Miao(), Si Yaochen, Sun Honggang, Li Hong-xia(), Du Yihao, Shang Xinlian   

  1. State Key Laboratory of Advanced Refractories,Sinosteel Luoyang Institute of Refractories Research Co.,Ltd.,Luoyang 471039,Henan,China
  • Received:2020-07-28 Online:2021-08-15 Published:2021-08-22
  • Contact: Li Hong-xia

MgAlON及其复合材料研究进展

夏淼(), 司瑶晨, 孙红刚, 李红霞(), 杜一昊, 尚心莲   

  1. 中钢集团洛阳耐火材料研究院有限公司 先进耐火材料国家重点实验室 河南洛阳 471039

Abstract:

The current research status of preparing MgAlON materials by carbon thermal nitriding method,solid phase reaction method,direct nitriding method and discharge plasma sintering method was reviewed in China and overseas,and the development direction of MgAlON materials was prospected.

Key words: MgAlON, composite materials, preparation method, review

摘要:

综述了国内外利用碳热还原氮化法、固相反应法、直接氮化法及放电等离子烧结法制备MgAlON材料的研究现状,并展望了MgAlON材料的发展方向。

关键词: MgAlON, 复合材料, 制备方法, 研究进展

CLC Number: