Refractories ›› 2022, Vol. 56 ›› Issue (2): 174-179.DOI: 10.3969/j.issn.1001-1935.2022.02.018

Previous Articles     Next Articles

Research progress on preparation of BN porous ceramics

Zhang Xin(), Han Lei, Wu Shuaibing, Cai Wejie, Zhang Haijun()   

  1. The State Key Laboratory of Refractories and Metallurgy,Wuhan University of Science and Technology,Wuhan 430081,Hubei,China
  • Received:2021-09-03 Online:2022-04-15 Published:2022-04-21
  • Contact: Zhang Haijun

BN多孔陶瓷的制备研究进展

张鑫(), 韩磊, 吴帅兵, 蔡伟杰, 张海军()   

  1. 武汉科技大学 省部共建耐火材料与冶金国家重点实验室 湖北武汉 430081
  • 通讯作者: 张海军
  • 作者简介:张鑫:男,1999年生,硕士研究生。E-mail: 2016634419@qq.com
  • 基金资助:
    国家自然科学基金面上项目(51872210);国家自然科学基金面上项目(52072194);湖北省教育厅高等学校优秀中青年科技创新团队计划项目(T201602)

Abstract:

BN porous ceramics have great application potential in fields such as adsorption,heat insulation,environmental repairing,and electronic packaging owing to their high porosity,high specific surface area,low thermal conductivity,and excellent chemical stability.The recent progress on the preparation of BN porous ceramics was briefly summarized.The structure and performance of BN porous ceramics prepared by template and non-template methods as well as the advantages and disadvantages of these methods were sketched.The challenges and future development direction on the preparation and application of BN porous ceramics were proposed.

Key words: boron nitride porous ceramics, preparation method, template method, non-template method

摘要:

BN多孔陶瓷因具有高孔隙率、高比表面积、低热导率、优异的化学稳定性等优点,在吸附、保温隔热、环境修复及电子包装等领域应用潜力巨大。简要综述了近年来BN多孔陶瓷制备方法的进展,概述了模板法与非模板法所制备BN多孔陶瓷的结构及性能,总结了各种制备方法的优缺点,提出了BN多孔陶瓷制备及其应用方面所面临的挑战和未来的发展方向。

关键词: BN多孔陶瓷, 制备方法, 模板法, 非模板法

CLC Number: