Refractories ›› 2025, Vol. 59 ›› Issue (2): 177-184.DOI: 10.3969/j.issn.1001-1935.2025.02.016

Previous Articles    

Research progress on preparation of sheet-like silicon nitride ceramics by tape-casting technology

Zhao Chenxiao, Li Shipeng, Wang Gang, Zhou Yudong, Yuan Bo   

  1. First author’s address:State Key Laboratory of Advanced Refractories,Sinosteel Luoyang Institute of Refractories Research Co.,Ltd.,Luoyang 471039,Henan,China
  • Received:2024-08-07 Online:2025-04-15 Published:2025-04-14

流延成型技术制备片状氮化硅陶瓷研究进展

赵辰啸, 李世鹏, 王刚, 周玉栋, 袁波   

  1. 中钢集团洛阳耐火材料研究院有限公司 先进耐火材料全国重点实验室 河南洛阳 471039
  • 通讯作者: 袁波,男,1983年生,博士,高级工程师。E-mail:boyuan0401@163.com
  • 作者简介:赵辰啸:男,2000年生,硕士研究生。E-mail:15530090311@163.com

Abstract: The principles and processes of preparing silicon nitride ceramics by tape-casting technology in China and aboard were reviewed.The characteristics of various additives in both organic and water-based tape-casting slurry systems as well as the influence of process parameters on the tape-casting effect were elaborated.The research progress and existing problems in the preparation of sheet-like silicon nitride ceramics by tape-casting technology were summarized.The future development direction of this technology was discussed.

Key words: silicon nitride ceramics, tape-casting, organic tape-casting system, water-based tape-casting system

摘要: 综述了国内外关于流延成型技术制备氮化硅陶瓷的原理和流程,阐述了有机和水基流延浆料体系中各种添加剂的特点和工艺流程参数对流延效果的影响,总结了流延成型技术制备片状氮化硅陶瓷的研究进展及仍存在的问题,同时探讨该技术未来的发展方向。

关键词: 氮化硅陶瓷, 流延成型, 有机流延体系, 水基流延体系