Effect of magnesium lactate and magnesium gluconate on hydration behavior of light-burnt magnesia

Zhou Jing, Wang Zhoufu, Liu Hao, Ma Yan, Xia Zhongfeng, Quan Zhenghuang, Deng Chengji   

  1. First author's address:State Key Laboratory of Advanced Refractories,Wuhan University of Science and Technology,Wuhan 430081,Hubei,China
  • Received:2024-11-14 Online:2025-08-15 Published:2025-08-18

乳酸镁和葡萄糖酸镁对轻烧MgO水化行为的影响

周晶, 王周福, 刘浩, 马妍, 夏忠锋, 全正煌, 邓承继   

  1. 武汉科技大学 先进耐火材料全国重点实验室 湖北武汉 430081
  • 作者简介:周晶:女,1999年生,硕士研究生。E-mail:1977255385@qq.com
  • 基金资助:
    国家自然科学基金区域联合基金项目(U20A20239);国家自然科学基金(52372031)。

Abstract: To optimize its hydration behavior,light-burnt magnesia was used as the raw material,with magnesium lactate and magnesium gluconate as retarders.The hydration degree,hydration heat,and 1H-NMR of the light-burnt magnesia were characterized to study the effects of the two retarders on the setting time and the microscopic morphology of the hydration products of the light-burnt magnesia.The results show that,compared with magnesium lactate,magnesium gluconate has a more significant effect on the hydration,the hardening behavior,and the microscopic morphology of the hydration products of the light-burnt MgO.With 3 mass% magnesium lactate,the cumulative heat release after 50 h of hydration is approxi-mately 400 J·g-1,the initial setting time is 15 min,and the hydration products exhibit lamellar petal-like crystal morphology.With 3 mass% magnesium gluconate,the cumulative heat release after 50 h of hydration is approximately 300 J·g-1,the initial setting time extends to 45 min,and the hydration products show hexagonal plate-like or tetragonal bipyramidal crystal morphology.

Key words: light-burnt magnesia, retarder, hydration behavior, magnesium lactate, magnesium gluconate