Abstract:

The application and research state of TiO2 in Al2O3-SiO2,MgO-Al2O3,and carbon containing systems as well as monolithic refractories were overviewed to provide references for the further application of TiO2 in refractories.

Key words: titania, refractories application, research progress

摘要:

综述了TiO2在Al2O3-SiO2系、MgO-Al2O3系、含碳材料以及不定形耐火材料等方面的应用和研究现状,以期为TiO2在耐火材料中的进一步应用提供参考。

关键词: 二氧化钛, 耐火材料应用, 研究进展