Refractories ›› 2022, Vol. 56 ›› Issue (1): 88-92.DOI: 10.3969/j.issn.1001-1935.2022.01.019

Previous Articles    

Application progress of dolomite

Wang Shaoyang1)(), Qi Xin1), Luo Xudong1)(), Jing Changsheng2), Li Zhen3)   

  1. 1)School of Materials and Metallurgy,University of Science and Technology Liaoning,Anshan 114051,Liaoning,China
  • Received:2021-05-13 Online:2022-02-15 Published:2022-02-24
  • Contact: Luo Xudong

白云石的应用进展

王少阳1)(), 祁欣1), 罗旭东1)(), 井长胜2), 李振3)   

  1. 1)辽宁科技大学 材料与冶金学院 辽宁鞍山 114051
    2)辽宁省国家新材料工程建设中心 辽宁沈阳 110032
    3)营口理工学院 辽宁营口 115014
  • 通讯作者: 罗旭东
  • 作者简介:王少阳:男,1999年生,硕士研究生。E-mail: 544024236@qq.com
  • 基金资助:
    国家自然科学基金联合基金资助项目(U1908227);国家自然科学基金联合基金资助项目(U20A20239)

Abstract:

The extensive application of dolomite in the fields such as refractories and magnesium smelting was reviewed.The challenges and in-depth research direction of dolomite in the future were pointed out.

Key words: dolomite, refractories, building materials, chemical industry, metallurgy, application

摘要:

综述了白云石在耐火材料、镁冶炼等领域的广泛应用,指出了白云石未来所面临的挑战和深入研究的方向。

关键词: 白云石, 耐火材料, 建材, 化工, 冶金, 应用