Application progress of h-BN in refractories and high temperature ceramics for metallurgy

He Yuanhang, Qian Fan, Guo Hairong, Li Hualong, Lu Yue, Liu Guoqi, Li Hongxia   

  1. First author’s address:State Key Laboratory of Advanced Refractories,Sinosteel Luoyang Institute of Refractories Research Co.,Ltd.,Luoyang 471039,Henan,China
  • Received:2022-08-24 Online:2023-08-15 Published:2023-08-30

h-BN在耐火材料和冶金用高温陶瓷中的应用进展

贺远航1), 钱凡1), 郭海荣2), 李化龙2), 路跃1), 刘国齐1), 李红霞1)   

  1. 1)中钢集团洛阳耐火材料研究院有限公司 先进耐火材料国家重点实验室 河南洛阳 471039
    2)江苏省沙钢钢铁研究院有限公司 江苏苏州 215625
  • 作者简介:贺远航:男,1997年生,硕士研究生。E-mail:3537982669@qq.com
  • 基金资助:
    国家重点研发计划项目(2021YFB3701400)。

Abstract: h-BN has excellent thermal shock resistance and chemical stability.It has a graphite-like layered structure and is widely used in metallurgy,chemical industry,electronics and other fields.The research and application of h-BN in refractories were reviewed,including the improvement of the thermal shock resistance,oxidation resistance,and slag resistance of refractories by h-BN,as well as its effect on the sintering properties of refractories.The application of hot-pressed sintered h-BN composites in key components of iron and steel metallurgy and the improvement measures of the mechanical properties,thermal shock resistance,oxidation resistance and corrosion resistance to molten steel were summarized.The problems existing in the application of h-BN in refractories and high temperature ceramics for metallurgy were pointed out.

Key words: h-BN, graphite, thermal shock resistance, oxidation resistance, slag resistance, corrosion resistance to molten steel

摘要: h-BN具有优异的抗热震性和化学稳定性,具有类石墨层状结构,在冶金、化工、电子等领域应用广泛。综述了h-BN在耐火材料中的研究应用情况,包括h-BN对耐火材料抗热震性、抗氧化性和抗渣性的改善,以及对耐火材料烧结性的影响;概述了热压烧结h-BN复合材料在钢铁冶金关键部件的应用及其力学性能、抗热震性、抗氧化性和抗钢液侵蚀性的改善措施;指出了h-BN在耐火材料及冶金用高温陶瓷应用中存在的问题。

关键词: h-BN, 石墨, 抗热震性, 抗氧化性, 抗渣性, 抗钢液侵蚀性