Refractories ›› 2023, Vol. 57 ›› Issue (4): 365-368.DOI: 10.3969/j.issn.1001-1935.2023.04.019

Previous Articles    

Interaction between vanadium titanomagnetite slag and refractories

Gao Wei, Liu Zhaoyang, Ma Beiyue, Wei Shan, Yu Jingkun   

  1. First author’s address:School of Metallurgy,Northeastern University,Shenyang 110819,Liaoning,China
  • Received:2022-07-28 Online:2023-08-15 Published:2023-08-30

钒钛磁铁矿熔渣与耐火材料间的相互作用

高伟1), 刘朝阳1), 马北越1), 韦善2), 于景坤1)   

  1. 1)东北大学 冶金学院 辽宁沈阳 110819
    2)攀钢集团钒钛资源股份有限公司 四川攀枝花 617000
  • 作者简介:高伟:女,1996年生,硕士研究生。E-mail:aw2020211@163.com
  • 基金资助:
    国家自然科学基金(52004058);中国博士后科学基金(2020M670776)。

Abstract: The interaction between titanium slag or vanadium slag formed during smelting vanadium titanomagnetite in the blast furnace-converter process and refractories was analyzed and summarized.The corrosion process and mechanism of refractories for iron and steel smelting by titanium slag and vanadium slag were pointed out,and the occurrence state of variable valence metal elements,such as vanadium,titanium and iron in vanadium-titanium slag was explored.It was proposed that using computer simulation and other auxiliary technologies to analyze the corrosion behavior of refractories by a complex slag system would be the future development direction.

Key words: titanium slag, vanadium slag, refractories, corrosion

摘要: 分析总结了高炉-转炉工艺冶炼钒钛磁铁矿过程中形成的钛渣和钒渣与耐火材料间的相互作用,指出了钢铁冶炼用耐火材料受钛渣和钒渣的侵蚀过程及机制,探究了钒、钛和铁等变价金属元素在钒钛渣中的赋存状态,提出了利用计算机模拟仿真等辅助技术分析复杂渣系对耐火材料的侵蚀行为将是未来的发展方向。

关键词: 钛渣, 钒渣, 耐火材料, 侵蚀

CLC Number: