| [1] |
Wei Jintao, Luo Yixin, Yang Bolin, Liu Zhenglong, Deng Luopeng, Yu Chao, Deng Chengji, Wang Zhoufu, Ding Jun.
Effect of La2O3 on mechanical properties and slag corrosion resistance of MgO-Mg2SiO4 refractories
[J]. Refractories, 2025, 59(2): 111-117.
|
| [2] |
Xue Junzhu, Liu Guangping, Chen Junfeng, Wei Guoping, Cheng Yaping, Yan Wen, Li Nan.
Influence of spinel addition on microstructure and properties of corundum-spinel castables
[J]. Refractories, 2025, 59(2): 155-161.
|
| [3] |
Xue Haitao, Liu Xingyu, Chen Ding, Gu Huazhi, Li Shaofei, Huang Ao, Fu Lyuping, Wu Shujun.
High-temperature water vapor corrosion resistance of Y2Si2O7 reinforced SiC based refractories
[J]. Refractories, 2025, 59(1): 8-12.
|
| [4] |
Luo Yixin, Wang Xing, Liu Zhenglong, Yu Chao, Deng Chengji, Ding Jun.
Effect of h-BN on properties of low carbon Al2O3-C refractories
[J]. Refractories, 2025, 59(1): 13-18.
|
| [5] |
Qu Xiaorui, Chen Liugang, Liu Ping, Gao Guangze, Fu Qiqi, Zhang Lixin.
Corrosion of high level radioactivity waste borosilicate liquid glass on chrome corundum refractories
[J]. Refractories, 2025, 59(1): 31-37.
|
| [6] |
Li Rui, Song Bo, Ma Shulong, Gao Changhe, Tian Lin, Li Guohua, Zhang Furong.
Influence of surface modifiers on properties of anti-corrosion coatings for cement kilns
[J]. Refractories, 2025, 59(1): 59-64.
|
| [7] |
Zou Zehui, Tong Shengli, Zhu Ziyun.
Effects of high titanium slag addition on properties of Al2O3-SiC-C castables
[J]. Refractories, 2025, 59(1): 76-81.
|
| [8] |
Qu Chao, Li Hang, Huang Xiaoyang, Zhang Haijun, Zhang Shaowei.
Research progress of refractories for cement rotary kilns
[J]. Refractories, 2025, 59(1): 87-92.
|
| [9] |
.
Effect of Cr2AlC on service performance of self-bonded SiC refractories
[J]. Refractories, 2024, 58(6): 480-485.
|
| [10] |
.
Pressureless in-situ synthesis of MgAlON composites from spent slide bricks and spent MgO-C bricks
[J]. Refractories, 2024, 58(6): 501-505.
|
| [11] |
.
Pressureless in-situ synthesis of MgAlON composites from spent slide bricks and spent MgO-C bricks
[J]. Refractories, 2024, 58(6): 506-512.
|
| [12] |
.
Research progress on slag resistance of different basic refractories
[J]. Refractories, 2024, 58(6): 527-535.
|
| [13] |
Deng Lina, Yi Shuai, Xue Fei, Pan Chuancai, Xu Qian, Jiang Chen, Bai Yaning.
Alkali vapor corrosion resistance of refractories for oxy-fuel combustion glass furnace
[J]. Refractories, 2024, 58(5): 440-444.
|
| [14] |
Gao Yunqin, Guo Kaige, Ma Aiqiong, Niu Xingrong, Yang Guang, Zhang Xudong.
Preparation and alkali corrosion resistance of mullite-corundum-magnesium aluminate spinel multiphase materials
[J]. Refractories, 2024, 58(4): 334-340.
|
| [15] |
Li Fei, Zhou Hui, Yang Zhichao, Tang Zhongdui, Wang Zhengfang, Liu Wei.
Corrosion mechanism of working lining of refining ladle wall with different molding methods
[J]. Refractories, 2024, 58(4): 344-348.
|