Refractories ›› 2026, Vol. 60 ›› Issue (1): 74-77.DOI: 10.3969/j.issn.1001-1935.2026.01.014
Previous Articles Next Articles
Li Dongmei, Li Guimei, Yan Lin, Li Hongchao, Li Lu, Ye Qing, Shao Changbo, Chen Zhiqiang
Received:
Online:
Published:
李冬梅, 李桂梅, 颜林, 李红超, 李璐, 叶青, 邵长波, 陈志强
通讯作者:
作者简介:
Abstract: Corundum castables often exhibit a decline in strength during medium and low temperature stages of baking and field application,which adversely affects their overall performance.To solve this problem,an optimization of the particle gradation by using multi-graded alumina ultrafines was proposed to enhance the structural stability and mechanical properties of the castables after medium and low temperature heat treatment.With tabular corundum and six types of alumina ultrafines with varying particle sizes (d50 of 3.910,1.885,1.362,1.104,0.798,and 0.524 μm,respectively) as the main raw materials,a five fraction gradation was designed.Its effects on the cold modulus of rupture (CMOR),permanent linear change on heating,and microstructure were systematically investigated.The results show that:(1)the samples with one-fraction or two-fraction gradation of ultrafines exhibit a significant decrease in cold modulus of rupture after heat treatment at 600 ℃ compared with those treated at 110 and 400 ℃;(2)the samples with a five-fraction gradation of ultrafines demonstrate stable performance in cold modulus of rupture within the 400-1 200 ℃ range,significantly mitigating the strength drop problem commonly encountered around 600 ℃ in traditional single-ultrafine systems.Meanwhile,the high-temperature-treated samples present a denser microstructure and more stable permanent linear change on heating.This study provides an effective strategy for optimizing the medium and low temperature performance of corundum castables,demonstrating a good engineering application value.
Key words: corundum castables, alumina ultrafines, multi-fraction gradation, cold modulus of rupture, permanent linear change on heating
摘要: 刚玉浇注料在烘烤和现场使用过程中,常在中低温阶段出现强度下降,影响其整体使用性能。为解决该问题,提出采用多级氧化铝微粉进行粒度配比优化,以提升浇注料在中低温热处理后的结构稳定性和力学性能。选用板状刚玉和6种不同粒径的氧化铝微粉(d50分别为3.910、1.885、1.362、1.104、0.798和0.524 μm)为主原料,设计了5级配比制备刚玉浇注料,研究其对浇注料常温抗折强度、加热永久线变化率及其显微结构的影响。结果表明:采用一级和二级微粉配比的试样经600 ℃热处理后比110、400 ℃热处理后的常温抗折强度显著下降;采用5级微粉配比的试样在400~1 200 ℃的常温抗折强度表现稳定,显著改善了传统单一微粉体系在600 ℃附近出现的强度下降问题,同时,高温处理后显微结构更致密,加热永久线变化率更稳定。该研究为优化刚玉浇注料的中低温性能提供了有效思路,并具有良好的工程应用价值。
关键词: 刚玉浇注料, 氧化铝微粉, 多级配比, 常温抗折强度, 加热永久线变化率
CLC Number:
TQ175
Li Dongmei, Li Guimei, Yan Lin, Li Hongchao, Li Lu, Ye Qing, Shao Changbo, Chen Zhiqiang. Effect of multi-fraction gradation of alumina ultrafines on medium and low temperature properties of corundum castables[J]. Refractories, 2026, 60(1): 74-77.
李冬梅, 李桂梅, 颜林, 李红超, 李璐, 叶青, 邵长波, 陈志强. 氧化铝微粉多级配比对刚玉浇注料中低温性能的影响[J]. 耐火材料, 2026, 60(1): 74-77.