Refractories ›› 2021, Vol. 55 ›› Issue (1): 81-88.DOI: 10.3969/j.issn.1001-1935.2021.01.018

Previous Articles     Next Articles

Research progress of MgO-ZrO2 refractories

Ling Yongyi(), Wang Zhen, Zhang Jing, Wang Zihao, Liu Xinhong()   

  1. Henan Key Laboratory of High Temperature Functional Ceramics,Zhengzhou University,Zhengzhou 450052,Henan,China
  • Received:2020-05-30 Online:2021-02-15 Published:2021-02-15
  • Contact: Liu Xinhong

MgO-ZrO2质耐火材料研究进展

凌永一(), 王珍, 张婧, 王子昊, 刘新红()   

  1. 郑州大学 河南省高温功能材料重点实验室 河南郑州 450052
  • 通讯作者: 刘新红
  • 作者简介:凌永一:女,1996年生,硕士研究生。E-mail: lingyongyi0528@163.com
  • 基金资助:
    国家自然科学基金资助项目(51672253);国家自然科学基金资助项目(51872266)

Abstract:

The research progress of MgO-ZrO2 refractories was summarized in this paper.The emphasis was focused on the influences of the types of zirconia sources and their amount as well as additives on the performance,the composition and the microstructure of MgO-ZrO2 refractories.It was expected to provide technical data for the production and application of MgO-ZrO2 refractories.

Key words: magnesia-zirconia refractories, zirconia source, additives

摘要:

综述了镁锆质耐火材料的研究现状,重点介绍了引入锆源的种类、加入量及添加剂对镁锆质耐火材料性能、组成和结构的影响,期望为镁锆质耐火材料的生产和应用提供参考。