Refractories ›› 2021, Vol. 55 ›› Issue (2): 169-173.DOI: 10.3969/j.issn.1001-1935.2021.02.017

Previous Articles     Next Articles

Research progress of dense magnesia and porous magnesia materials

Ma Beiyue(), Zhang Yuzhong, Gao Zhi, Zhang Shuhao   

  1. School of Metallurgy,Northeastern University,Shenyang 110819,Liaoning,China
  • Received:2020-06-16 Online:2021-04-15 Published:2021-04-15

致密与多孔氧化镁材料研究进展

马北越(), 张誉忠, 高陟, 张书豪   

  1. 东北大学 冶金学院 辽宁沈阳 110819
  • 作者简介:马北越:男,1978年生,博士,副教授。E-mail:maby2005@126.com
  • 基金资助:
    东北大学第十四批(2020年)大学生创新训练计划(200094);NSFC-辽宁联合基金重点项目(U1908227)

Abstract:

Dense magnesia materials and porous magnesia materials are important branches of magnesia materials,and have played important roles in many important fields.The novel dense or porous magnesia materials are current research hotspots.The preparation progresses of dense magnesia materials and porous magnesia materials,the influence of different catalysts on dense magnesia materials were reviewed.Finally,some suggestions on the development of magnesia materials were put forward.

Key words: dense magnesia, additives, porous magnesia, research progress

摘要:

致密氧化镁材料和多孔氧化镁材料是氧化镁材料的重要组成部分,分别在不同的领域有关键作用,新型致密或多孔氧化镁材料是当下的研究热点。为此,主要综述了制备致密氧化镁材料的研究进展,不同催化剂对致密氧化镁材料的影响和制备多孔氧化镁材料的研究进展。最后对氧化镁材料的发展提出几点建议。

关键词: 致密氧化镁, 添加剂, 多孔氧化镁, 研究进展

CLC Number: