Refractories ›› 2026, Vol. 60 ›› Issue (1): 78-81.DOI: 10.3969/j.issn.1001-1935.2026.01.015
Previous Articles Next Articles
Guo Yong, Zhu Yi, Yu Qiwen, Fu Xiao-yong, Xiao Xiong
Received:
Online:
Published:
郭勇, 朱义, 余其文, 傅小勇, 肖雄
作者简介:
Abstract: To enhance the durability and reduce the cost of magnesia-based coatings for continuous casting tundishes,magnesia-based tundish coating materials were prepared using olivine,medium-grade magnesia clinker,and silica fume as the main raw materials,with magnesium sulfate heptahydrate as the binder.The effects of olivine additions (38%,45%,53%,61%,and 69%,by mass) on the phase composition,physical properties,and slag resistance of the coatings were researched.The results show that:(1)after heat treatment at 1 550 ℃,the main crystalline phases of the samples are periclase,forsterite,and stishovite.With the increasing olivine addition,the periclase content gradually decreases,while the forsterite and stishovite contents gradually increase;(2)at high temperatures,the magnesium ferrite and forsterite formed in the matrix exert a filling effect,leading to an increase in the bulk density and a decrease in the apparent porosity of the samples after heat treatment;(3)the expansive effect associated with the oxidation of FeO derived from the decomposition of fine olivine particles,coupled with the filling and strengthening effect of magnesium ferrite and forsterite on the matrix,results in unstable variation trends of the permanent linear change on heating and the cold compressive strength of the samples in different stages;(4)when the olivine addition is 61%,the coating exhibits the optimal slag resistance after being heat-treated at 1 550 ℃.
Key words: olivine, tundish, magnesia-based coatings, slag resistance
摘要: 为了提高连铸中间包镁质涂抹料的耐用性和降低其造价,以橄榄石、中档镁砂以及SiO2微粉为主原料,七水硫酸镁为结合剂制备了中间包用镁质涂抹料。研究了橄榄石添加量(添加质量分数分别为38%、45%、53%、61%、69%)对镁质涂抹料的物相组成、物理性能以及抗渣侵蚀性的影响。结果表明:1)经1 550 ℃热处理后,试样的主晶相为方镁石、镁橄榄石以及斯石英,并随橄榄石添加量的增加,方镁石逐渐减少,而镁橄榄石和斯石英逐渐增加;2)高温下基质中反应生成的铁酸镁和镁橄榄石对基质具有填充作用,使得试样热处理后的体积密度增加,显气孔率下降;3)细小颗粒橄榄石分解产生的FeO氧化而伴随的膨胀效应,以及铁酸镁和镁橄榄石对基质的填充增强作用,使得试样的加热永久线变化和常温耐压强度在不同区段变化趋势不稳定;4)当橄榄石添加量为61%(w)时,1 550 ℃热处理后涂抹料表现出最优异的抗渣性能。
关键词: 橄榄石, 中间包, 镁质涂抹料, 抗渣性
CLC Number:
TQ175
Guo Yong, Zhu Yi, Yu Qiwen, Fu Xiao-yong, Xiao Xiong. Effects of olivine additions on properties of magnesia-based coatings[J]. Refractories, 2026, 60(1): 78-81.
郭勇, 朱义, 余其文, 傅小勇, 肖雄. 橄榄石添加量对镁质涂抹料性能的影响[J]. 耐火材料, 2026, 60(1): 78-81.