耐火材料 ›› 2024, Vol. 58 ›› Issue (4): 307-313.DOI: 10.3969/j.issn.1001-1935.2024.04.006

• 研究开发 • 上一篇    下一篇

氧化铝粒径和氧化锆粉外加量对氧化铝造粒粉性能的影响

邓江1), 刘学新2), 李文2), 张子翼2), 员文杰1,3,4)   

  1. 1)武汉科技大学 省部共建耐火材料与冶金国家重点实验室 湖北武汉 430081
    2)湖北斯曼新材料股份有限公司 湖北黄冈 438400
    3)武汉科技大学 高温材料与炉衬技术国家地方联合工程研究中心 湖北武汉 430081
    4)武汉科技大学 钢铁工业耐火材料新技术国际合作联合实验室 湖北武汉 430081
  • 收稿日期:2024-01-12 出版日期:2024-08-15 发布日期:2024-08-21
  • 通讯作者: 员文杰,男,1980年生,博士,教授。E-mail:yuanwenjie@wust.edu.cn
  • 作者简介:邓江:男,1999年生,硕士研究生。E-mail:1261188641@qq.com

Effects of alumina particle size and zirconia powder extra-addition on sintering property of alumina granulated powder

Deng Jiang, Liu Xuexin, Li Wen, Zhang Ziyi, Yuan Wenjie   

  1. First author's address: The State Key Laboratory of Refractories and Metallurgy,Wuhan University of Science and Technology,Wuhan 430081,Hubei,China
  • Received:2024-01-12 Online:2024-08-15 Published:2024-08-21

摘要: 为了提高氧化锆增韧氧化铝(ZTA)造粒粉的烧结性能,以不同粒径(d50=1.72 μm,d50=3.48 μm,d50=13 nm)的Al2O3粉和氧化钇稳定氧化锆粉(YSZ)为主要原料,并加入黏结剂和分散剂,混合球磨得到ZTA浆料。研究了不同YSZ外加量(外加质量分数分别为0、5%、10%、15%和20%)对浆料流变性能的影响。并采用喷雾干燥法制备了ZTA造粒粉。造粒粉经压样成型后分别在1 520、1 600和1 680 ℃保温2 h烧成,并测试其线收缩率和致密度。结果表明:1)ZTA浆料呈现剪切变稀的特性,并且具有一定的屈服应力,浆料的流变性能符合Herschel-Bulkley模型,拟合的相关系数较高,>0.98;2)所制备的ZTA造粒粉的粒度分布范围主要在125~45 μm,粒度分布较广;3)以99%(w)活性Al2O3粉(d50=1.72 μm)为主要原料,加入1%(w)纳米Al2O3(d50=13 nm)、外加15%(w)YSZ时,所制备造粒粉性能较好,其对应的卡尔系数为8.62%,含水率为0.22%,休止角为25.2°,经1 600 ℃保温2 h烧后,其致密度为94.8%,线收缩率为18.2%。

关键词: 喷雾干燥法, 氧化锆增韧氧化铝(ZTA), 流变性能, 致密度, 线收缩率

Abstract: This work aims at improving the sintering property of zirconia toughened alumina (ZTA) granulated powder.ZTA slurries were prepared through ball milling using alumina powder with different particle sizes (d50:1.72 μm,3.48 μm and 13 nm) and yttria stabilized zirconia (YSZ) as the main starting materials,adding binders and dispersants.The effect of the YSZ extra-addition (0,5%,10%,15% and 20%,by mass) on the rheological property of the slurries was investigated.ZTA granulated powders were prepared using the spray drying method,and then the powders were pressed into shapes and fired at different temperatures (1 520,1 600,and 1 680 ℃).The linear shrinkage and relative density of the fired samples were determined.The results show that:(1)the ZTA slurries exhibit shear thinning behavior and possess a yield stress;the rheological properties of the slurries are well-described by the Herschel-Bulkley model,with a high correlation coefficient (>0.98);(2)the particle size of the prepared ZTA granulated powders is mainly within the range of 125 to 45 μm,demonstrating a wide distribution;(3)the optimal formulation is 99 mass% activated alumina powder (d50=1.72 μm),1 mass% nano-alumina (d50=13 nm),and 15 mass% YSZ (extra-adding);this formulation results in a Carr coefficient of 8.62%,a water content of 0.22%,and an angle of repose of 25.2°;after firing at 1 600 ℃ for 2 h,the sample exhibits a relative density of 94.8% and a linear shrinkage rate of 18.2%.

Key words: spray drying method, zirconia toughened alumina (ZTA), rheological property, relative density, linear shrinkage