Refractories ›› 2021, Vol. 55 ›› Issue (1): 30-34.DOI: 10.3969/j.issn.1001-1935.2021.01.007

Previous Articles     Next Articles

Effect of carbon black on pore structure of lightweight homogenized bauxite

Zhu Huiliang1)(), Liu Yan2), Ren Bo2), Sang Shaobai2), Zhu Huang2)   

  1. 1)Yixing Products Quality & Foods Safety Inspection & Testing Center,Jiangsu Ceramics Refractory Products Quality Supervision & Inspection Center,Yixing 214205,Jiangsu,China
  • Received:2020-09-18 Online:2021-02-15 Published:2021-02-15

炭黑对轻量均化矾土孔结构的影响

朱惠良1)(), 刘燕2), 任博2), 桑绍柏2), 朱煌2)   

  1. 1)宜兴市产品质量和食品安全检验检测中心 江苏省陶瓷耐火材料产品质量监督检验中心江苏宜兴 214205
    2)武汉科技大学 省部共建耐火材料与冶金国家重点实验室 湖北武汉 430081
  • 作者简介:朱惠良:男,1966年生,高级工程师。E-mail: 18018309325@163.com
  • 基金资助:
    国家重点研发计划项目(2019YFC1904900);湖北省自然科学基金杰出青年人才项目(2019CFA050);江苏省市场监管局科技计划项目(KJ207507)

Abstract:

Lightweight homogenized bauxite samples were prepared with homogenized bauxite raw powder and carbon black.The effects of the carbon black type (N990 and N774),the carbon black addition (0,4%,and 8%,by mass),and the heat-treatment temperature (1 450,1 500,and 1 550 ℃ for 3 h) on the pore structure of the lightweight homogenized bauxite were investigated.The results reveal that with the heat-treatment temperature increasing,the pore amount in the lightweight homogenized bauxite decreases but the average pore diameter increases;pores in the samples with N990 exhibit more uniform distribution and smaller average size since N990 is easy to disperse;while the average pore size distribution of the samples with N774 is less uniform and the average pore size increases with the rising N774 addition since N774 is not easy to disperse.

Key words: lightweight, homogenized bauxite, carbon black, pore structure

摘要:

以均化矾土生料和炭黑为主要原料,研究了炭黑种类(炭黑N990和炭黑N774)、加入量(加入质量分数分别为0、4%和8%)及热处理温度(1 450、1 500和1 550 ℃下保温3 h)对轻量均化矾土孔结构的影响。结果表明:随着温度的升高,轻量均化矾土气孔数量逐渐减少,平均孔径增大;炭黑N990易于分散,所制得的轻量均化矾土气孔分布均匀且孔径尺寸相对较小;炭黑N774粒子难以均匀分散,所制得的轻量均化矾土孔径分布不规律,且其平均孔径随加入量增加而明显增大。