Refractories ›› 2022, Vol. 56 ›› Issue (3): 267-271.DOI: 10.3969/j.issn.1001-1935.2022.03.021

Previous Articles     Next Articles

Research progress on refractories for inclined channel area of CDQ ovens and their damage mechanism

Han Cangjuan1)(), Zhang Meijie2)   

  1. 1)MCC5 Group Shanghai Co.,Ltd.,Shanghai 201999,China
  • Received:2021-10-09 Online:2022-06-15 Published:2022-06-24

干熄焦炉斜道区耐火材料及损毁机制研究进展

韩藏娟1)(), 张美杰2)   

  1. 1)五冶集团上海有限公司 上海 201999
    2)武汉科技大学 材料与冶金学院 湖北武汉 430081
  • 作者简介:韩藏娟:女,1983年生,博士,工程师。E-mail: 282882443@qq.ocm

Abstract:

The research progress of refractories for inclined channel area of CDQ ovens and their damage mechanism in recent years was reviewed.The advantages and disadvantages of the research were summarized.The research direction and development trend of the inclined channel area of CDQ ovens were prospected.

Key words: coke dry quenching oven, inclined channel area, refractories, damage mechanism

摘要:

综述了近些年来干熄焦炉斜道区耐火材料的研究现状及损毁机制的研究进展,总结了现有研究的优点和不足,展望了干熄焦炉斜道区研究方向和发展趋势。

关键词: 干熄焦炉, 斜道区, 耐火材料, 损毁机制