Refractories ›› 2022, Vol. 56 ›› Issue (6): 511-514.DOI: 10.3969/j.issn.1001-1935.2022.06.011

Previous Articles     Next Articles

Current air pollutant emission situation and control measures of refractory industry in Henan Province

Zhang Aiqin, Wang Haozhao, Cao Xia, Deng Huaxiang, Pang Long, Cao Jiahui   

  1. College of Materials and Chemical Engineering,Zhengzhou University of Light Industry,Zhengzhou 450002,Henan,China
  • Received:2022-01-05 Online:2022-12-15 Published:2022-12-26

河南省耐火材料行业大气污染物排放现状及治理措施研究

张爱勤1), 王号召1), 曹霞1), 邓华翔2), 庞龙1), 曹佳慧1)   

  1. 1)郑州轻工业大学 材料与化学工程学院 河南郑州 450002
    2)新密市生态环境监测站 河南新密 452370
  • 作者简介:张爱勤:女,1978年生,博士,副教授。E-mail:zhangaiqin@zzuli.edu.cn
  • 基金资助:
    生态环境部大气重污染成因与治理攻关项目(DQGG202136)。

Abstract: Based on the investigation of over 1 400 refractory enterprises in Henan Province,the current situation of air pollutant emission was analyzed from the aspects of online monitoring and detection of air pollutant emission amount and concentration,and the pollution control process of refractory enterprises using different types of furnaces was summarized and analyzed.According to the survey results,the problems existing in the prevention and control of air pollutants in refractory enterprises in Henan Province were discussed.Simultaneously,corresponding pollution control measures were proposed,which could provide references and ideas for promoting the pollution reduction of refractory industry in Henan Province and formulating relevant pollutant emission standards.

Key words: refractories, air pollutant, current emission situation, control measures

摘要: 通过对河南省1 400余家耐火材料企业的调研,从企业大气污染物排放量、污染物排放浓度在线监测与检测情况等方面分析了河南省耐火材料行业大气污染物排放现状,并对使用不同类型炉窑的耐火材料企业的污染治理工艺进行汇总和分析;根据调研结果探讨了目前河南省耐火材料企业在大气污染物防治方面存在的问题,并提出了相应的污染治理措施,为促进河南省耐火材料工业污染减排、制订相关污染物排放标准提供借鉴和思路。

关键词: 耐火材料, 大气污染物, 排放现状, 治理措施