Refractories ›› 2026, Vol. 60 ›› Issue (5): 430-435.DOI: 10.3969/j.issn.1001-1935.2026.05.010

Previous Articles     Next Articles

Industrial air pollutant emission limits of refractories for different kiln temperatures

Sun Peng, Sun Hanghang, Deng Huaxiang, Xu Yuanqian, Yan Yali, Bai Ling, Cao Xia   

  1. First author’s address:College of Materials and Chemical Engineering,Zhengzhou University of Light Industry,Zhengzhou 450001,Henan,China
  • Received:2025-12-09 Online:2026-10-15 Published:2026-10-29

基于不同窑温的耐火材料工业大气污染物排放限值探讨

孙鹏1), 孙航航1), 邓华翔2), 徐媛倩1), 闫亚丽3), 白玲1), 曹霞1)   

  1. 1)郑州轻工业大学 材料与化学工程学院 河南郑州 450001
    2)郑州市生态环境监测和安全中心 河南郑州 450007
    3)河南省化工研究所有限责任公司 河南郑州 450052
  • 作者简介:孙鹏:男,1985年生,硕士,高级工程师。E-mail:2021603@zzuli.edu.cn
  • 基金资助:
    大气重污染成因与治理攻关项目(No.DQGG202136);河南省科技攻关项目(242102320152);河南省自然科学基金资助项目(252300420874);郑州轻工业大学博士科研基金项目(2022BSJJZK11)。

Abstract: As a key process parameter for the firing of refractories,kiln temperature directly affects the generation and emission of air pollutants such as NOx,SO2,VOCs and particulate matter.This work aims to systematically analyze the variation characteristics of air pollutant concentrations in refractories industry kilns under different firing temperatures,so as to provide scientific references for the green upgrading and pollution emission reduction of the industry.Taking Henan Province as an example,the development status of the refractories industry and the generation-emission characteristics of major pollutants were firstly summarized,and then the stack emission limits of air pollutants under different kiln temperature conditions were determined.The results show that the emission limit of particulate matter for refractories industry is 10 mg·m-3;and that of SO2 is 50 mg·m-3.There is a significant positive correlation between NOx concentration and kiln temperature.The NOx emission limit is 50 mg·m-3 for kilns operating at 300-1 200 ℃,100 mg·m-3 for 1 200-1 700 ℃,200 mg·m-3 for kilns with temperatures above 1 700 ℃,and 300 mg·m-3 for high-temperature electric smelting furnaces with temperatures exceeding 2 000 ℃.The emission limit of non-methane total hydrocarbons (NMHC) is 30 mg·m-3.

Key words: refractories, kiln temperature, emission limits, air pollutants

摘要: 窑温作为耐火材料烧成的重要工艺参数,直接影响着大气污染物(NOx、SO2、VOCs、颗粒物等)的产生与排放。为了系统分析耐火材料行业窑炉不同烧成温度下大气污染物浓度变化特征,从而为行业绿色升级及污染减排提供科学参考,以河南省为例,对河南省耐火材料行业发展现状和主要污染物产排特征进行了总结,并基于不同窑温条件确定了大气污染物有组织排放限值。结果表明:耐火材料工业的颗粒物排放限值为10 mg·m-3;SO2排放限值为50 mg·m-3;NOx浓度与窑温的正相关显著,窑温在300~1 200 ℃的NOx排放限值为50 mg·m-3,窑温1 200~1 700 ℃的NOx排放限值为100 mg·m-3,窑温大于1 700 ℃的NOx排放限值为200 mg·m-3,高温电熔炉窑温达到2 000 ℃以上的NOx排放限值为300 mg·m-3;非甲烷总烃排放限值为30 mg·m-3。

关键词: 耐火材料, 窑温, 排放限值, 大气污染物