耐火材料 ›› 2023, Vol. 57 ›› Issue (5): 446-451.DOI: 10.3969/j.issn.1001-1935.2023.05.016

• 综合评述 • 上一篇    下一篇

含锆耐火材料的研究进展

张艳利, 彭西高, 张小会, 程庆先, 王晓利   

  1. 中钢集团洛阳耐火材料研究院有限公司 河南洛阳 471039
  • 收稿日期:2023-05-29 出版日期:2023-10-15 发布日期:2023-10-26
  • 作者简介:张艳利:女,1982年生,硕士,高级工程师。E-mail:smile8200@163.com

Research progress on zirconia-containing refractories

Zhang Yanli, Peng Xigao, Zhang Xiaohui, Cheng Qing-xian, Wang Xiaoli   

  1. First author's address: Sinosteel Luoyang Institute of Refractories Research Co.,Ltd.,Luoyang 471039,Henan,China
  • Received:2023-05-29 Online:2023-10-15 Published:2023-10-26

摘要: 综述了高锆质材料、含锆镁质材料、含锆钙质材料、含锆刚玉质材料及非氧化物-ZrO2复合耐火材料的研究概况,发现:1)合理选择ZrO2原料的稳定剂类型,可以有效改善高锆质耐火材料的抗热震性能并提高使用寿命;2)预合成原料(镁锆砂、CaZrO3、锆莫来石、造粒氧化锆微粉和Zr(OH)4凝胶等)和轻质含ZrO2原料(ZrO2空心球微珠等)可以在镁质、钙质及刚玉质耐火材料中取得较好的应用效果;3)锆英砂适用于制备非氧化物-ZrO2复合材料及部分不定形耐火材料。基于此,提出了含锆耐火材料未来需要重点关注的研究方向。

关键词: ZrO2, 含锆镁质材料, 含锆钙质材料, 含锆刚玉质材料, SiAlON-ZrO2复合材料

Abstract: The research progress of high-zirconia refractories,zirconia-containing magnesia refractories,zirconia-containing calcia refractories,zirconia-containing corundum refractories and non-oxides-ZrO2 composite refractories was reviewed.It is found that:(1)the reasonable selection of stabilizers for ZrO2 raw materials can effectively improve the thermal shock resistance of high-zirconia refractories and prolong the service life;(2)pre-synthetic raw materials (such as magnesia zirconia sand,CaZrO3,zirconia-mullite,granulated zirconia micropowder and Zr(OH)4 gel) and lightweight zirconia-containing raw materials (such as zirconia hollow beads) perform good application effects in magnesia refractories,calcia refractories and corundum refractories;(3)zircon sand is suitable for preparing non-oxides-ZrO2 composites and some monolithic refractories.Based on this,the research direction of zirconia-containing refractories in the future was put forward.

Key words: zirconia, zirconia-containing magnesia refractories, zirconia-containing calcia refractories, zirconia-containing corundum refractories, SiAlON-ZrO2 composites