Refractories ›› 2021, Vol. 55 ›› Issue (5): 381-384.DOI: 10.3969/j.issn.1001-1935.2021.05.002

Previous Articles     Next Articles

Reflection on science and technology innovation of refractories under carbon emission peak and carbon neutrality background

Li Hongxia()   

  1. Sinosteel Luoyang Institute of Refractories Research Co.,Ltd.,Luoyang 471039,Henan,China
  • Received:2021-07-31 Online:2021-10-15 Published:2021-10-25

双碳背景下耐火材料科技创新的思考

李红霞()   

  1. 中钢集团洛阳耐火材料研究院有限公司 河南洛阳 471039
  • 作者简介:李红霞:女,1965年生,博士,教授级高级工程师。E-mail: lihongx0622@126.com

Abstract:

ased on the carbon emission peak and neutrality targets,the carbon reduction and green development situation of main high-temperature industries were introduced.The new technologies for pollution and carbon reduction in the iron and steel industry were emphasized.The challenges and opportunities for refractories industry under the double carbon targets were analyzed,and the main innovation directions of refractories were pointed out.

Key words: carbon emission peak, carbon neutrality, refractories, science and technology innovation, carbon reduction and green development

摘要:

基于“碳达峰”和“碳中和”的双碳目标,介绍了双碳背景下耐火材料所服务的主要高温行业减碳绿色发展的形势,重点介绍了钢铁行业双碳目标下减污降碳新技术,以及与之相适应的耐火材料科技创新的重点,分析了双碳目标下耐火材料行业的挑战和机遇,指出了耐火材料科技创新的主要方向。

关键词: 碳达峰, 碳中和, 耐火材料, 科技创新, 减碳绿色发展